Hi Sebastian,
Is I0 the same for all measurements? Mu being about the same jump just
means that about
the same amount of absorber is in the beam. It doesn't rule out an
instrumentation issue.
Start by checking I0, then It. Identify where the noise is manifesting.
-R.
On 2024-04-29 5:17 a.m., Sebastian Kunze wrote:
> Greetings, I recently did in-situ QEXAFS at Ag K-edge, expecting to
> see structure loss starting from crystalline (metallic) state. While
> we can see that, in addition we also see an increase in noise(?) in
> the xanes region (compare start and
> ZjQcmQRYFpfptBannerStart
> This Message Is From an External Sender
> This message came from outside your organization.
> ZjQcmQRYFpfptBannerEnd
> Greetings,
>
> I recently did in-situ QEXAFS at Ag K-edge, expecting to see structure
> loss starting from crystalline (metallic) state. While we can see
> that, in addition we also see an increase in noise(?) in the xanes
> region (compare start and end in the attached image). I am confused by
> this because the amount of material did not change, so I did not
> expect a difference in the signal/noise ratio at the absorption edge.
> And it is reproducible across several samples, so not instrument
> related. Could anyone point me in the right direction as to what I am
> missing?
>
> Thank you!
>
> Best,
> Sebastian Kunze
>
>
> _______________________________________________
> Ifeffit mailing list
> Ifeffit at millenia.cars.aps.anl.gov
> https://urldefense.us/v3/__http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit__;!!G_uCfscf7eWS!fWsYAatgn9ghAnT9beKT8yAAdkY4UjnsDGG080jsUw76VDZAoZDTiDI_qaSCUuY_fLrv2AkFwkuGCjPlklxylreS7W6N1PJeOOg1qZM$
> Unsubscribe:https://urldefense.us/v3/__http://millenia.cars.aps.anl.gov/mailman/options/ifeffit__;!!G_uCfscf7eWS!fWsYAatgn9ghAnT9beKT8yAAdkY4UjnsDGG080jsUw76VDZAoZDTiDI_qaSCUuY_fLrv2AkFwkuGCjPlklxylreS7W6N1PJea47y2ig$
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20240429/8a99a15a/attachment.htm>
More information about the Ifeffit
mailing list