Joyti,
The coordination number of Rh-C bonds is defined as the total number of
Rh-C bonds in the sample divided by the total number of Rh atoms in the
sample.
Anatoly
-------------------------------------------------------------------
Anatoly I. Frenkel
Professor
Department of Materials Science and Chemical Engineering (primary
appointment)
Department of Chemistry (affiliate appointment)
Stony Brook University
Stony Brook, NY 11794
Email: anatoly.frenkel at stonybrook.edu
<https://mail.bnl.gov/OWA/redir.aspx?C=F6wCGt4adziN6IvpdRQ-rWdgy3Oaoif_x-0ybKTBGBlALcrWeszTCA..&URL=mailto%3ajgchen%40columbia.edu>
http://you.stonybrook.edu/frenkel
Co-Director and Spokesperson, Synchrotron Catalysis Consortium (SCC) at BNL
http://you.stonybrook.edu/scc2
Joint Appointment:
Senior Chemist
Chemistry Division, Brookhaven National Laboratory
Upton, NY 11973. Ph: 631-344-3013. Group: 631-344-3494
Email: frenkel at bnl.gov
https://www.bnl.gov/staff/frenkel
-------------------------------------------------------------------
On Mon, Apr 24, 2023 at 12:25 PM Jyoti Pandey <jyotipandey51092 at gmail.com>
wrote:
> Hello everyone,
>
> I have a cluster of 13 Rh atoms above the graphene sheet. The first
> coordination number that I am getting is around 1.65 (which is obtained by
> choosing a Rh-C) path. I am curious to know whether this value is the
> "exact" or the "average" coordination number w.r.t all the Rh atoms.
>
> Thanks
>
> With Best Regards
>
> Dr. Jyoti Pandey, Ph.D.
> Postdoctoral Researcher
> Department of Physics
> Central Michigan University, MI, USA
> Mobile No. +1-928-265-0599
> .....................................
>
> _______________________________________________
> Ifeffit mailing list
> Ifeffit at millenia.cars.aps.anl.gov
> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
> Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20230424/d72ca3af/attachment.htm>
More information about the Ifeffit
mailing list