[Ifeffit] Substrate material question
Jeff Terry
terryj at iit.edu
Tue Apr 27 10:32:00 CDT 2004
Hi Matt,
Both items are good to know. I didn't realize that the laminated kapton
structures still had good heat resistance.
Jeff
On Apr 27, 2004, at 10:22 AM, Matt Newville wrote:
> Hi Paul,
>
> I think you can get polyimide thicker than 175 microns. It may not
> go as Kapton, but maybe as Cirlex or Torlon or something else. I
> think goodfellow.com carries these in millimeter thick sheets and
> rods, and that they're still radiation and heat resistant.
> Goodfellow tends to be pricey, but has excellent information on
> thermal and mechanical properties.
>
> Using MgO, sapphire, or even diamond might be reasonable too.
>
> --Matt
>
> PS: I have a working build of PGPLOT with all of Aquaterm, X11,
> Postscript, and Png devices on Mac OS X. I'm still tweaking
> the makefile so that it links directly to the png objects to
> avoid possible conflicts with dynamic png and zlib libraries,
> but I should have a working ifeffit binary using this in a
> matter of days, and then be ready to tweak horae's Makefile.PL
> so that horae_update works.
>
>
> _______________________________________________
> Ifeffit mailing list
> Ifeffit at millenia.cars.aps.anl.gov
> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
More information about the Ifeffit
mailing list