12 Oct
2009
12 Oct
'09
7:26 p.m.
Hello all, Our group will be looking at the Ag L-edge soon. I wondered if anyone might have and share some data on Ag nanoparticles. We are running out of time and having trouble synthesizing small size (5-20nm) particles for comparison to our samples of interest. We will be collecting many Ag(salt) Cl, No3, So4 standards if anyone may be in need of those. Buena Salud, Chris Patridge Graduate Student Cell: 315-529-0501