Does anyone have EXAFS data to at least k=12 for Cr selenide of known phase? I'm working on fitting the EXAFS of Cr doped into Bi2Se3, and using Feff6L, the S02 comes out to 0.65 if I assume a substitutional site, which seems a bit low. mam