17 Aug
2006
17 Aug
'06
6:58 a.m.
hi everybody, does anyone have a literature reference explaining the shoulder in the XANES spectrum of HfO2 after the white line at about 9.58 keV. I think it is related to the number of oxygens coordinating, but i could not find any note about it by browsing the journals.... thanks very much! matthias -- Matthias Bauer Universität Stuttgart Institut für Physikalische Chemie Arbeitskreis Prof. Dr. H. Bertagnolli Pfaffenwaldring 55 70569 Stuttgart (Vaihingen) Telefon: (+49) 0711-685-4472 Fax: (+49) 0711-685-4443 E-Mail: m.bauer@ipc.uni-stuttgart.de homepage: http://www.ipc.uni-stuttgart.de/~matthias/index.htm
7044
Age (days ago)
7044
Last active (days ago)
0 comments
1 participants
participants (1)
-
m.bauer