13 Jan
2009
13 Jan
'09
9:15 p.m.
THank JeongEunSuk , Thank you for your suggestion, I will try to fitting it again. I just recheck the XRD result. I got a only 1 sharp peak at 002 (31.311 degree) which represent a WZ structure, but you are talking about atomic disorder. Could you describe about this difference. -- Mr. Kittiphong Amnuyswat [kaswat] Post Graduate student College of KMITL Nanotechnology Contact : kaswat@gmail.com, nakz_zz@hotmail.com [MSN Available]