Dear Colleagues, I would like to measure some Gold-Nanoparticles that are embedded in a kind of polymer-matrix consisting of a polystyrene-core and some polyelectrolyte-chains. The total amount of gold in the suspension will be 0.025-0.05 percent by weight. The idea is to place the sample in a polystyrene cuvette with approximately 1 mm diameter (sample) and (2x) 1 mm (polystyrene). We've tried once to measure in transmission mode, where we had some problems maybe due to the absorption of water and polystyrene. Measurements in fluorescence mode might also cause problems by self-absorption and the absorption of the polystyrene again. Does anybody have good experience with liquid measurements of diluted samples? Best regards, Julian ========================================= Julian Kaiser Helmholtz-Zentrum Berlin für Materialien und Energie Hahn-Meitner-Platz 1, D-14109 Berlin Tel. +49 30 8062 - 43029 Mail: Julian.Kaiser@helmholtz-berlin.de ========================================= Helmholtz-Zentrum Berlin für Materialien und Energie GmbH Mitglied der Hermann von Helmholtz-Gemeinschaft Deutscher Forschungszentren e.V Vorsitzender des Aufsichtsrats: Prof. Dr. Dr. h.c. mult. Joachim Treusch Stellvertretende Vorsitzende: Dr. Beatrix Vierkorn-Rudolph Geschäftsführer: Prof. Dr. Anke Rita Kaysser-Pyzalla, Prof. Dr. Dr. h.c. Wolfgang Eberhardt, Dr. Ulrich Breuer Sitz der Gesellschaft: Berlin Handelsregister: AG Charlottenburg, 89 HRB 5583 =========================================