Have you read the Colinet & Pasturel paper? Skimming through it, it seems like section III.b along with Fig 1 gives enough information to fill in the Atoms window (http://bruceravel.github.io/demeter/documents/Artemis/feff/index.html) by hand. B On 08/08/2016 05:02 PM, Ed Han wrote:
Dear All,
In the upcoming fall, my research group plans on performing XAS studies observing the Hf L3-edge for various Hf-Al intermetallic samples.
In preparation for the experiments, I am looking for CIF files of the various Hf-Al intermetallic systems, including HfAl3, HfAl2, Hf4Al3, etc.
Upon scavenging through a multitude of crystallographic databases, I was not able to find any CIF files of Hf-Al intermetallics. However, I have acquired powder diffraction files (PDF) for said intermetallics.
Seeing as how PDFs cannot be used in Artemis for EXAFS data analysis (to my knowledge), is there a way to convert PDFs into CIFs? I have attached one of the PDF files to demonstrate what information it contains.
I would really appreciate your help!
Regards, Edmund Han
_______________________________________________ Ifeffit mailing list Ifeffit@millenia.cars.aps.anl.gov http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit
-- Bruce Ravel ------------------------------------ bravel@bnl.gov National Institute of Standards and Technology Synchrotron Science Group at NSLS-II Building 743, Room 114 Upton NY, 11973 Homepage: http://bruceravel.github.io/home/ Software: https://github.com/bruceravel Demeter: http://bruceravel.github.io/demeter/