13 Aug
2006
13 Aug
'06
6:41 p.m.
Dear All, Does someone happen to have a data set of Zr k- edge in metallic glass alloy, either with Pt or Cu? I just collected some data of Zr3Pt1 metallic glass ribbon in transmission and the spectrum looks wired...... Thanks, Ning Yang