24 Nov
2018
24 Nov
'18
10:25 a.m.
Enyuan,
Here are the rutile and anatase spectra with the corresponding Ti foil
spectrum.
I will send you the name of a student who collected the spectra for
acknowledgement when you need it.
Anatoly Frenkel
On Fri, Nov 23, 2018 at 10:08 PM Enyuan Hu
Hi all,
Can anyone share an XAS spectrum of TiO2? it would be best if a Ti foil spectrum is also included for calibration. Your help is much appreciated!
Enyuan _______________________________________________ Ifeffit mailing list Ifeffit@millenia.cars.aps.anl.gov http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit