Dear Mohamed,
I think you will have some kind of "over" or "self" -absorption from the
substrate, specially in geometries other than grazing incidence. I have
performed that kind of experiments in fluorescence and in transmission. The
result was that the absorption coefficient signal I was interested in,
really was of 2nd or 3rd order of magnitud less that the "tail" of
absorption of the substrate. I would not do that again. Maybe somebody has
better experience.
Regards
Maria Elena
2010/11/16 mohamed sobhy
Dear All I would like to grow UO2 thin films on STO (SrTiO3) substrate but I found that Sr K-edge 16105 and U L3-edge is 17166. Do you think there will be any interference? Best,
Mohamed