Dear All, Recently, i have performed EXAFS for YbVO4 bulk (prepared through sintering process) and nanoparticles (at room temperature). Nanoparticles were synthesized by co-precipitation technique and their EXAFS was measured by passing the prepared solution using peristaltic pump. After all subtraction (background and solvent), nanoparticles XAS data were recovered and processed for the fitting. After Fourier transform, it was observed that both nanoparticles posses an additional short peak (or shoulder) at about 1.2 A from bulk. Since the peak appears much closer to 1 A, i suspect this may due to artifact or bad background subtraction. Hence, i would like to know the way to eliminate this peak at short distance. Regards, Raj