Hi Peng,
See
http://cars9.uchicago.edu/ifeffit/FAQ/Data_Handling#How_can_I_read_data_file...
I believe there is a plugin for reading these files in (D)Athena.
--Matt
On Wed, Jul 30, 2014 at 9:54 PM, Peng Liu
Hi all,
I searched the Farel Lytle Database and looked like I found chalcopyrite spectra for Cu from http://ixs.iit.edu/database/data/Farrel_Lytle_data/RAW/Cu/index.html.
I downloaded the data, but I can not import into Athena. I looked into the data, it looked wired for me. The first column doesn't look like energy for Cu.
I am wondering if anyone have any idea how to import or transfer the data. I attached the data file.
Regards,
Peng
-- Ph.D. Candidate Earth and Environmental Sciences, CEIT Bldg. Rm. 2026 University of Waterloo Ph: 519-888-4567 ext. 37232 200 University Avenue West Waterloo, Ontario N2L 3G1 Fax:519-746-3882p26liu@uwaterloo.ca
_______________________________________________ Ifeffit mailing list Ifeffit@millenia.cars.aps.anl.gov http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit