On 08/28/2013 03:31 PM, mattie.peck@huskers.unl.edu wrote:
I'm using the new version of Artemis to open old .apj files and when I try to run a fit the program completely shuts down. It allows me to start Artemis and load plots but as soon as I click the "fit" button it crashes. I have attached the .apj file and the dartemis log file and I have copied the text from the log file below. I have the latest version of demeter 0.9.18 and I am running Windows XP.
Thanks for the help.
Yup. That's broken. It's not immediately obvious what the problem is. I'll let you know when I figure something out. B -- Bruce Ravel ------------------------------------ bravel@bnl.gov National Institute of Standards and Technology Synchrotron Science Group at NSLS --- Beamlines U7A, X24A, X23A2 Building 535A Upton NY, 11973 Homepage: http://xafs.org/BruceRavel Software: https://github.com/bruceravel