Hi Paul, I am sorry but I have never tried to evaporate anything onto it. Jeff Jeff Terry Biological, Chemical, and Physical Sciences Illinois Institute of Technology Chicago IL 60616 phone 630-252-9708 fax 630-252-0358 http://mrmac.mr.aps.anl.gov/~jterry/ On Apr 26, 2004, at 8:34 PM, Paul Fons wrote:
Wow that was fast. Thanks. Can you deposit something on it and have it stick? e.g. the idea is to deposit a thin film of a semiconductor on it and then place the film under biaxial stress to look at structural changes by xafs.
On Apr 27, 2004, at 10:24 AM, Jeff Terry wrote:
Hi Paul,
Kel-f is good to a little over 200 C. I have mm thicknesses of it.
http://www.boedeker.com/pctfe_p.htm
Jeff
Jeff Terry Biological, Chemical, and Physical Sciences Illinois Institute of Technology Chicago IL 60616 phone 630-252-9708 fax 630-252-0358 http://mrmac.mr.aps.anl.gov/~jterry/
On Apr 26, 2004, at 8:12 PM, Paul Fons wrote:
OK, I admit this isn't an athena question (but it is about how to take the raw data for it!). I want to do biaxial strain measurements. The idea is to deposit a thin film of the material to be investigated on a substrate and then deform the plate with a form of cylindrical symmetry. One can then solve for the stress of a plate using elasticity theory. The twist is that I need a plate that is stiff and (surprise) x-ray transparent ... and heat resistant to about 250 C. Kapton would be a wonderful choice, but is only made in thicknesses up to 175 microns (hardly stiff enough). There must be someone out there in the collective iffeffit world who knows of an appropriate material. Doing some web surfing, I came across another product by DuPont called Vespar that *may* be available in thicker forms. The specs I am looking for are: a thin (semiconducting) film has to stick to the surface, heat resistant to <=250 C, thick enough to be elastically stiff, and x-ray transparent. Any suggestions? Thanks for any help that may come my way in advance!
Dr. Paul Fons Senior Researcher National Institute for Advanced Industrial Science & Technology METI Center for Applied Near-Field Optics Research (CANFOR) AIST Central 4, Higashi 1-1-1 Tsukuba, Ibaraki JAPAN 305-8568
tel. +81-298-61-5636 fax. +81-298-61-2939
email: paul-fons@aist.go.jp
The lines below are in a Japanese font
〒305−8568 茨城県つくば市東1−1−1 つくば中央第4 近接場光応用工学センター ポール・フォンス主任研究官_______________________________________________ Ifeffit mailing list Ifeffit@millenia.cars.aps.anl.gov http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
_______________________________________________ Ifeffit mailing list Ifeffit@millenia.cars.aps.anl.gov http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
Dr. Paul Fons Senior Researcher National Institute for Advanced Industrial Science & Technology METI Center for Applied Near-Field Optics Research (CANFOR) AIST Central 4, Higashi 1-1-1 Tsukuba, Ibaraki JAPAN 305-8568
tel. +81-298-61-5636 fax. +81-298-61-2939
email: paul-fons@aist.go.jp
The lines below are in a Japanese font
〒305−8568 茨城県つくば市東1−1−1 つくば中央第4 近接場光応用工学センター ポール・フォンス主任研究官 _______________________________________________ Ifeffit mailing list Ifeffit@millenia.cars.aps.anl.gov http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit