18 Jan
2021
18 Jan
'21
10:07 p.m.
Dear all, Firstly I would like to wish you a much better year than in 2020. Does anyone have some spectra of nanocrystalline NiO (not bulk standards)? I have a spectrum of a mixed compound and would like to get more insights into what I really have in this sample. Thank you in advance!!! Kind regards, -- *Christian Wittee Lopes* *Visiting Researcher* ANP/FINEP - PRH50 Institute of Chemistry, Universidade Federal do Rio Grande do Sul (UFRGS) Phone: +55 54 992430264