-----Original Message----- From: ifeffit-bounces@millenia.cars.aps.anl.gov [mailto:ifeffit- bounces@millenia.cars.aps.anl.gov] On Behalf Of Jens Kruse Sent: Wednesday, January 10, 2007 8:56 AM To: ifeffit@millenia.cars.aps.anl.gov Subject: [Ifeffit] Problems with the >flatten< option in Athena
Hi,
I have a normalization problem with Athena. If I turn on the "flatten" option in the background removal section, Athena creates in some of
Hi Jens, You can try moving e0. E0 should be on the edge. Is E0 at the position of the step? You could also send us an example. Then we can help more directly. I'd guess that the step is caused by some background parameters that are set incorrectly. SK the
normalized spectra a step in the pre-edge range. How can I get rid of it?
Thanks,