W dniu 12-12-12 18:49, Matthew Marcus pisze:
I have never tried fitting peak shapes to the Bragg peaks (say, a Lorentzian or pseudo-Voight plus a smooth polynomial; don't subtract the polynomial). I have never tried too, simply I took care of data during experiment, as is mentioned in posts before. And I suppose it would be very painful, more than Pb tape... Anyway - good ideal with this Pb tape.
coming back to the problem with Bragg peaks, does anyone knows if it is possible to analyse EXAFS with more than 1 interest regions? like 2 or more FT windows - before, between and after Bragg peaks, or is possible to introduce one own FT window function in Athena? regards kicaj