Hi Bruce, I installed the new horae (035) and played around with the ZnO tutorial using the new version of Artemis. I called the program in the directory where the ZnO dat file reside from the command line. The project apj1 (run with all the indications in the journal) worked smoothly. As soon as I try to read in the apj2, the following trap message pops up: # Artemis 0.7.005 # This file created at 00:19:09 on 31 May, 2004 # using darwin, perl 5.008001, Tk 804.027, and Ifeffit 1.2.5 # Workspace: /Users/stefano/.horae/stash/artemis.project.3/ The following message was trapped by Artemis on a SIGWARN: Artemis0.7.005warn/Users/stefano/.horae/stash/ARTEMIS.TRAPCODE(0x1e3dff8)/Users/stefano/.horae/stash/artemis.project.3/ at /Applications/Ifeffit/bin/artemis line 1562 main::__ANON__('Tk::Error: could not open /Users/stefano/.horae/stash/artemis...') called at blib/lib/Tk.pm (autosplit into blib/lib/auto/Tk/Error.al) line 488 Tk::Error('MainWindow=HASH(0x8f44c)','could not open /Users/stefano/.horae/stash/artemis.project.3/...','main::nnnn_header at /Applications/Ifeffit/bin/artemis line 4386','main::read_path at /Applications/Ifeffit/bin/artemis line 10872','main::open_project at /Applications/Ifeffit/bin/artemis line ...','main::read_data at /Applications/Ifeffit/bin/artemis line 6901','main::dispatch_read_data at /Applications/Ifeffit/bin/artemis...','main::__ANON__ at /Applications/Ifeffit/bin/artemis line 586','Tk callback for ..frame.menubutton.menu.project_data',...) called at /Library/Perl/5.8.1/darwin-thread-multi-2level/Tk.pm line 406 eval {...} called at /Library/Perl/5.8.1/darwin-thread-multi-2level/Tk.pm line 406 Tk::MainLoop() called at /Applications/Ifeffit/bin/artemis line 1707 End of trap file. Exactly the SAME error message pops out when I try to save a fit as chi(k). Obviously I am stuck... Any help here? Again, there must be some problem with the perl libraries... HELP!!! Stefano -- ____________________________________________ Stefano Ciurli Professor of Chemistry Department of Agro-Environmental Science and Technology University of Bologna Viale Giuseppe Fanin, 40 I-40127 Bologna Italy Phone: +39-051-209-6204 Fax: +39-051-209-6203 "Fatti non foste a viver come bruti, ma per seguir virtute e canoscenza" Dante Alighieri - Inferno - Canto XXVI -- ____________________________________________ Stefano Ciurli Professor of Chemistry Department of Agro-Environmental Science and Technology University of Bologna Viale Giuseppe Fanin, 40 I-40127 Bologna Italy Phone: +39-051-209-6204 Fax: +39-051-209-6203 "Fatti non foste a viver come bruti, ma per seguir virtute e canoscenza" Dante Alighieri - Inferno - Canto XXVI