On Monday 15 May 2006 03:40, you wrote:
Dear Bruce, I have some problems with the occupation probability which it is in the publication. To take into account of this factor, A solution is to remove manually the atoms (the half for an occupation of 1/2) but is there such possiblity in the Atoms program?
Dominique, This is perhaps the most frequent of the frequently asked questions. See FAQ #14 at this page: http://cars9.uchicago.edu/iffwiki/FAQ/FeffitModeling B -- Bruce Ravel ---------------------------------------------- bravel@anl.gov Molecular Environmental Science Group, Building 203, Room E-165 MRCAT, Sector 10, Advanced Photon Source, Building 433, Room B007 Argonne National Laboratory phone and voice mail: (1) 630 252 5033 Argonne IL 60439, USA fax: (1) 630 252 9793 My homepage: http://cars9.uchicago.edu/~ravel EXAFS software: http://cars9.uchicago.edu/~ravel/software/