Dear all, I'm trying to fit the Fe K-edge EXAFS data and I appreciate that Fe in my sample mainly exists as Fe4+, which is associated with Jahn-Teller distortion. The one shell model that considers Fe residing in the standard octahedral apparently didn't give satisfactory result. I'm sorry that even though I found people do fitting considering Jahn-Teller distortion, I am still not aware of how to carry that out in Artemis. Can someone helps me to look at my fitting and give me some guidance on how to implement fitting that considers Jahn-Teller distortion in Artemis? Thank you. -- Enyuan