Sebastian,
What is happening “in situ”? Are you heating the sample, flowing gas, or changing some other external conditions?
The cleaner spectra are also those with larger oscillations, implying a more uniform local environment. That might suggest that the less clean spectra are from samples with more pinholes or non-uniformity in the bulk distribution of sample particles within the beam.
--Matt
From: Ifeffit on behalf of Sebastian Kunze
Date: Monday, April 29, 2024 at 8:21 AM
To: ifeffit@millenia.cars.aps.anl.gov
Subject: [Ifeffit] Origin of noise in Ag K-Edge
Greetings, I recently did in-situ QEXAFS at Ag K-edge, expecting to see structure loss starting from crystalline (metallic) state. While we can see that, in addition we also see an increase in noise(?) in the xanes region (compare start and
ZjQcmQRYFpfptBannerStart
This Message Is From an External Sender
This message came from outside your organization.
ZjQcmQRYFpfptBannerEnd
Greetings,
I recently did in-situ QEXAFS at Ag K-edge, expecting to see structure loss starting from crystalline (metallic) state. While we can see that, in addition we also see an increase in noise(?) in the xanes region (compare start and end in the attached image). I am confused by this because the amount of material did not change, so I did not expect a difference in the signal/noise ratio at the absorption edge. And it is reproducible across several samples, so not instrument related. Could anyone point me in the right direction as to what I am missing?
Thank you!