Hi Raheleh, We have submitted a bug fix for this. Expect a new version of Larch to be released shortly. We rely heavily on Larch for our EXAFS Neo analysis package and this has broken our code as well. Jeff Jeff Terry Interim Chair, Department of Social Sciences Professor of Physics Professor of Mechanical, Materials, and Aerospace Engineering Editor, Applied Surface Science Prairie Chapter Chair, AVS Illinois Institute of Technology 3101 S. Dearborn St. Chicago IL 60616 630-252-9708 Sent from my iPhone
On Oct 20, 2021, at 9:12 AM, Daneshpour, Raheleh
wrote: Hello!
I am Raheleh a PhD student at Penn State working in FeNi catalysis and using XAS. I am trying to install the Larch, but I constantly get an error message on different computers and using different installation methods. The attached file is a screenshot of the error message I got. Could you please help me to figure out how to solve the problem? Thanks, Raheleh
Raheleh Daneshpour (She/Her) Ph.d. student Email: rmd5926@psu.edu
Chemical engineering department The Pennsylvania State University University Park, PA
_______________________________________________ Ifeffit mailing list Ifeffit@millenia.cars.aps.anl.gov http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit