17 Dec
2018
17 Dec
'18
5:27 p.m.
Attached...foil measured simultaneously in transmission on 20BM at APS..only to about 12 invAng though. On 2018-12-17 9:08 a.m., Lorenzo Stievano wrote:
Hi everybody,
daes anybody have in his repository a Fe K-edge XAS spectrum of maghemite (gamma-Fe2O3)? I would need it as a reference material in a study on doped iron oxides.
Thanks a lot in advance!
Lorenzo
_______________________________________________ Ifeffit mailing list Ifeffit@millenia.cars.aps.anl.gov http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit