Alistair: I would think not since the edge shift depends on where the empty states are positioned relative to the Fermi energy and the fact that the symmetry is different for the L3 and L2 edges. The L1 is an s to p transition so it is even more different. Carlo On Thu, 20 Oct 2005, McCready, Alistair wrote:
OK, a theoretical question whose answer may be straight-forward (and I will probably ridiculed for such a simple question)!!
If you analyse, for example, the Pb L3 edge of 2 minerals and you then analyse the Pb L2 edge of the same 2 minerals, will the difference between the edges of 2 minerals be the same, irrespective of the edge you use?
Cheers Alistair ------------------------------------------ Dr. Alistair J. McCready Mining & Minerals Saskatchewan Research Council 125-15 Innovation Blvd. Saskatoon, SK, S7N 2X8 Canada
Tel: 306 933-7103 Fax: 306 933-7446 email: mccready@src.sk.ca
"SRC provides Smart Science Solutions"
This e-mail and any files transmitted with it are intended only for the named recipients and may contain legally privileged and/or confidential information. If you are not the intended recipient please do not disseminate, distribute or copy this e-mail without the consent of the sender.
-- Carlo U. Segre -- Professor of Physics Associate Dean for Special Projects, Graduate College Illinois Institute of Technology Voice: 312.567.3498 Fax: 312.567.3494 Carlo.Segre@iit.edu http://www.iit.edu/~segre