19 Sep
2009
19 Sep
'09
2:30 a.m.
Dear All, I am doing the analysis of some unknown cobalt-containing samples, and I suspect that there might be cobalt carbide there. Thus I am wondering if anybody has a cobalt K edge XANES spectrum of cobalt carbide to share. Your help will be greatly appreciated! Many thanks! Xiaoming Wang Yale University