It would help to attach your atoms file
Carlo
--
Carlo Segre
Professor of Physics
Illinois Institute of Technology
On Sep 9, 2010, at 2:29 PM, mohamed sobhy
Dear I would like to fit the signal from (U0.8Ce0.2)O2, so I tried to put Ce in the same position of U but all atoms generated files give no Ce in the scattering paths and some fitting give negative amplitude values. Could you help me with the Atoms input file?
Mohamed