Dear Bruce We have used Athena and Artemis software to analyses the EXAFS. When we do the analysis, we used different S2o for each path for fitting of Cu2O data. I succeeded to obtain good fitting by this way. Documents related to percent EXAFS analysis have been mentioned S2o is one value for all paths. What I want to know is our fittings are correct or not. I am looking forward early response. About 10 years ago we had being using another program made by Tokyo University in Japan. In this program, the refined parameters also included S2oj and Nj to the each cells Thanks Ruwn