<div dir="ltr">Friends in XAFS,<div><br></div><div>Do you have any EXAFS spectra of single-phase ZrO2 or HfO2 that you'd be willing to share?</div><div><br></div><div>In particular, I'm looking for the monoclinic (P21/c), tetragonal (P42/nmc), and orthorhombic (Pbca and Pca21) phases of each material. Bulk, interface-stabilized, pure, or lightly doped is fine. I'd prefer mu(E) spectra, but chi(k) would work as well.</div><div><br></div><div>Thank you for any help or recommendations!</div><div><br></div><div>Martin</div><div><br></div><div>Martin E. McBriarty, Ph.D.</div><div>Scientist III, Intermolecular Inc.<br></div><div>San Jose, CA</div></div>