<p dir="ltr">Hello Fuxiang,</p>
<p dir="ltr">A small suggestion</p>
<p dir="ltr">Please also don't forget to try multiple edge data fitting if you already measured your data in both Fe and Ni edge, this may actually reduce the number of parameters to use. You need just on parameter  Fe-Ni/Ni-Fe should be same when looking from both atom</p>
<p dir="ltr">Hope it helps,</p>
<p dir="ltr">Ditty</p>
<div class="gmail_quote">On Jun 23, 2016 23:48,  <<a href="mailto:ifeffit-request@millenia.cars.aps.anl.gov">ifeffit-request@millenia.cars.aps.anl.gov</a>> wrote:<br type="attribution"><blockquote class="gmail_quote" style="margin:0 0 0 .8ex;border-left:1px #ccc solid;padding-left:1ex">Send Ifeffit mailing list submissions to<br>
        <a href="mailto:ifeffit@millenia.cars.aps.anl.gov">ifeffit@millenia.cars.aps.anl.gov</a><br>
<br>
To subscribe or unsubscribe via the World Wide Web, visit<br>
        <a href="http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit" rel="noreferrer" target="_blank">http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit</a><br>
or, via email, send a message with subject or body 'help' to<br>
        <a href="mailto:ifeffit-request@millenia.cars.aps.anl.gov">ifeffit-request@millenia.cars.aps.anl.gov</a><br>
<br>
You can reach the person managing the list at<br>
        <a href="mailto:ifeffit-owner@millenia.cars.aps.anl.gov">ifeffit-owner@millenia.cars.aps.anl.gov</a><br>
<br>
When replying, please edit your Subject line so it is more specific<br>
than "Re: Contents of Ifeffit digest..."<br>
<br>
<br>
Today's Topics:<br>
<br>
   1. Re: How to input atoms in solid solution for Artemis<br>
      (Scott Calvin)<br>
   2. Re: How to input atoms in solid solution for Artemis<br>
      (Fuxiang Zhang)<br>
<br>
<br>
----------------------------------------------------------------------<br>
<br>
Message: 1<br>
Date: Thu, 23 Jun 2016 16:23:36 -0400<br>
From: Scott Calvin <<a href="mailto:dr.scott.calvin@gmail.com">dr.scott.calvin@gmail.com</a>><br>
To: XAFS Analysis using Ifeffit <<a href="mailto:ifeffit@millenia.cars.aps.anl.gov">ifeffit@millenia.cars.aps.anl.gov</a>><br>
Subject: Re: [Ifeffit] How to input atoms in solid solution for<br>
        Artemis<br>
Message-ID: <<a href="mailto:F8C55BBE-4E8E-436E-97C4-35387D9B5B02@gmail.edu">F8C55BBE-4E8E-436E-97C4-35387D9B5B02@gmail.edu</a>><br>
Content-Type: text/plain; charset="utf-8"<br>
<br>
One additional thought:<br>
<br>
Distinguishing Ni-Ni and Ni-Fe by creating two different feff paths and fitting the spectrum as a mixture of the two is very difficult, to put it mildly, as both Anatoly and Matt indicated.<br>
<br>
But the bond length determined by your fit may be able to give you a clue, particularly when compared to appropriate standards. Depending on the details of your structure, the average bond length may depend on the fraction of sites occupied by iron to a degree which is measurable by EXAFS. Even if you simply use a nickel-nickel scattering path in feff to model your structure, differences in bond length could be indicative of changes in site occupancy.<br>
<br>
Ideally, this could be done by creating a series of standards with known iron-nickel ratios, fitting the bond length for each, and then comparing a fit of a sample with a similar structure but unknown iron-nickel ratio to the results for the standards.<br>
<br>
?Scott Calvin<br>
Sarah Lawrence College<br>
<br>
> On Jun 23, 2016, at 3:41 PM, Fuxiang Zhang <<a href="mailto:zhangfx@umich.edu">zhangfx@umich.edu</a>> wrote:<br>
><br>
> Hi, Matt and Anayoly,<br>
> Thank you very much for the help.<br>
><br>
> Fuxiang<br>
><br>
> On Thu, Jun 23, 2016 at 1:51 PM, Anatoly I Frenkel <<a href="mailto:afrenke2@yu.edu">afrenke2@yu.edu</a> <mailto:<a href="mailto:afrenke2@yu.edu">afrenke2@yu.edu</a>>> wrote:<br>
> Whatever you decide to do, remember that Ni Ni and Ni Fe pairs look very similar by EXAFS, so it does not matter how you end up doing it.<br>
> You can as well use pure Ni but you may want to consider both fcc and bcc structure for making the model because the alloy may end up to be either that or that, especially if it is a nanoalloy.<br>
><br>
> Anayoly<br>
><br>
><br>
><br>
> Sent from my Verizon Wireless 4G LTE Tablet<br>
><br>
><br>
> -------- Original message --------<br>
> From: Fuxiang Zhang <<a href="mailto:zhangfx@umich.edu">zhangfx@umich.edu</a> <mailto:<a href="mailto:zhangfx@umich.edu">zhangfx@umich.edu</a>>><br>
> Date: 6/23/2016 12:51 PM (GMT-05:00)<br>
> To: <a href="mailto:ifeffit@millenia.cars.aps.anl.gov">ifeffit@millenia.cars.aps.anl.gov</a> <mailto:<a href="mailto:ifeffit@millenia.cars.aps.anl.gov">ifeffit@millenia.cars.aps.anl.gov</a>><br>
> Subject: [Ifeffit] How to input atoms in solid solution for Artemis<br>
><br>
> Hi, All,<br>
> I am new in using EXAFS techniques. Just wondering how to input atomic structure of NiFe solid solution to Artemis. It has a simple Ni-structure, but both Ni and Fe occupy the same site. If I use partial occupancy, Artemis program does not allow. Anyone can give me an ideal?<br>
> Also the coordination number N cannot be refined in this simple system (12), is that right? In fact I just want to get the N through the fitting of EXAFS because of the partial occupancy.<br>
> Thank you very much<br>
><br>
> Fuxiang Zhang<br>
><br>
> _______________________________________________<br>
> Ifeffit mailing list<br>
> <a href="mailto:Ifeffit@millenia.cars.aps.anl.gov">Ifeffit@millenia.cars.aps.anl.gov</a> <mailto:<a href="mailto:Ifeffit@millenia.cars.aps.anl.gov">Ifeffit@millenia.cars.aps.anl.gov</a>><br>
> <a href="http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit" rel="noreferrer" target="_blank">http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit</a> <<a href="http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit" rel="noreferrer" target="_blank">http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit</a>><br>
> Unsubscribe: <a href="http://millenia.cars.aps.anl.gov/mailman/options/ifeffit" rel="noreferrer" target="_blank">http://millenia.cars.aps.anl.gov/mailman/options/ifeffit</a> <<a href="http://millenia.cars.aps.anl.gov/mailman/options/ifeffit" rel="noreferrer" target="_blank">http://millenia.cars.aps.anl.gov/mailman/options/ifeffit</a>><br>
><br>
><br>
> _______________________________________________<br>
> Ifeffit mailing list<br>
> <a href="mailto:Ifeffit@millenia.cars.aps.anl.gov">Ifeffit@millenia.cars.aps.anl.gov</a><br>
> <a href="http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit" rel="noreferrer" target="_blank">http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit</a><br>
> Unsubscribe: <a href="http://millenia.cars.aps.anl.gov/mailman/options/ifeffit" rel="noreferrer" target="_blank">http://millenia.cars.aps.anl.gov/mailman/options/ifeffit</a><br>
<br>
-------------- next part --------------<br>
An HTML attachment was scrubbed...<br>
URL: <<a href="http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20160623/f98683ca/attachment-0001.html" rel="noreferrer" target="_blank">http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20160623/f98683ca/attachment-0001.html</a>><br>
<br>
------------------------------<br>
<br>
Message: 2<br>
Date: Thu, 23 Jun 2016 17:47:00 -0400<br>
From: Fuxiang Zhang <<a href="mailto:zhangfx@umich.edu">zhangfx@umich.edu</a>><br>
To: XAFS Analysis using Ifeffit <<a href="mailto:ifeffit@millenia.cars.aps.anl.gov">ifeffit@millenia.cars.aps.anl.gov</a>><br>
Subject: Re: [Ifeffit] How to input atoms in solid solution for<br>
        Artemis<br>
Message-ID:<br>
        <CAP=<a href="mailto:koc6bTHKqDGk30bqQPH%2B56apQ8Jn5g0gCxhMRJbqhMhc38A@mail.gmail.com">koc6bTHKqDGk30bqQPH+56apQ8Jn5g0gCxhMRJbqhMhc38A@mail.gmail.com</a>><br>
Content-Type: text/plain; charset="utf-8"<br>
<br>
Hi, Scott,<br>
<br>
In fact, I have a series of single crystal Ni-Fe alloys (Fm-3m) with known<br>
atomic ratio, and measured both Fe and Ni edges for samples and standards.<br>
I just want to see if there's any difference between the local bonding<br>
environment of Fe and Ni, such as R, N and sigma2. Now using the suggested<br>
method by Matt by changing atoms in FEFF.inp file, I can only get ss, deltr<br>
and E0 from fitting (I don't know how to refine N and R). But the fitting<br>
with Ni (or Fe) edge can only generate the same R and deltr for Ni-Ni and<br>
Ni-Fe pairs. Fitting the edges of Ni and Fe will yield a little difference<br>
in the R and deltr. Which results should I believe, or something wrong I am<br>
using the program because I cannot generate different R for Ni-Ni and Ni-Fe<br>
pairs with the same data set.<br>
Many thanks for your suggestions and helps.<br>
<br>
Fuxiang Zhang<br>
<br>
On Thu, Jun 23, 2016 at 4:23 PM, Scott Calvin <<a href="mailto:dr.scott.calvin@gmail.com">dr.scott.calvin@gmail.com</a>><br>
wrote:<br>
<br>
> One additional thought:<br>
><br>
> Distinguishing Ni-Ni and Ni-Fe by creating two different feff paths and<br>
> fitting the spectrum as a mixture of the two is very difficult, to put it<br>
> mildly, as both Anatoly and Matt indicated.<br>
><br>
> But the bond length determined by your fit *may* be able to give you a<br>
> clue, particularly when compared to appropriate standards. Depending on the<br>
> details of your structure, the average bond length may depend on the<br>
> fraction of sites occupied by iron to a degree which is measurable by<br>
> EXAFS. Even if you simply use a nickel-nickel scattering path in feff to<br>
> model your structure, differences in bond length could be indicative of<br>
> changes in site occupancy.<br>
><br>
> Ideally, this could be done by creating a series of standards with known<br>
> iron-nickel ratios, fitting the bond length for each, and then comparing a<br>
> fit of a sample with a similar structure but unknown iron-nickel ratio to<br>
> the results for the standards.<br>
><br>
> ?Scott Calvin<br>
> Sarah Lawrence College<br>
><br>
> On Jun 23, 2016, at 3:41 PM, Fuxiang Zhang <<a href="mailto:zhangfx@umich.edu">zhangfx@umich.edu</a>> wrote:<br>
><br>
> Hi, Matt and Anayoly,<br>
> Thank you very much for the help.<br>
><br>
> Fuxiang<br>
><br>
> On Thu, Jun 23, 2016 at 1:51 PM, Anatoly I Frenkel <<a href="mailto:afrenke2@yu.edu">afrenke2@yu.edu</a>><br>
> wrote:<br>
><br>
>> Whatever you decide to do, remember that Ni Ni and Ni Fe pairs look very<br>
>> similar by EXAFS, so it does not matter how you end up doing it.<br>
>> You can as well use pure Ni but you may want to consider both fcc and bcc<br>
>> structure for making the model because the alloy may end up to be either<br>
>> that or that, especially if it is a nanoalloy.<br>
>><br>
>> Anayoly<br>
>><br>
>><br>
>><br>
>> Sent from my Verizon Wireless 4G LTE Tablet<br>
>><br>
>><br>
>> -------- Original message --------<br>
>> From: Fuxiang Zhang <<a href="mailto:zhangfx@umich.edu">zhangfx@umich.edu</a>><br>
>> Date: 6/23/2016 12:51 PM (GMT-05:00)<br>
>> To: <a href="mailto:ifeffit@millenia.cars.aps.anl.gov">ifeffit@millenia.cars.aps.anl.gov</a><br>
>> Subject: [Ifeffit] How to input atoms in solid solution for Artemis<br>
>><br>
>> Hi, All,<br>
>> I am new in using EXAFS techniques. Just wondering how to input atomic<br>
>> structure of NiFe solid solution to Artemis. It has a simple Ni-structure,<br>
>> but both Ni and Fe occupy the same site. If I use partial occupancy,<br>
>> Artemis program does not allow. Anyone can give me an ideal?<br>
>> Also the coordination number N cannot be refined in this simple system<br>
>> (12), is that right? In fact I just want to get the N through the fitting<br>
>> of EXAFS because of the partial occupancy.<br>
>> Thank you very much<br>
>><br>
>> Fuxiang Zhang<br>
>><br>
>> _______________________________________________<br>
>> Ifeffit mailing list<br>
>> <a href="mailto:Ifeffit@millenia.cars.aps.anl.gov">Ifeffit@millenia.cars.aps.anl.gov</a><br>
>> <a href="http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit" rel="noreferrer" target="_blank">http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit</a><br>
>> Unsubscribe: <a href="http://millenia.cars.aps.anl.gov/mailman/options/ifeffit" rel="noreferrer" target="_blank">http://millenia.cars.aps.anl.gov/mailman/options/ifeffit</a><br>
>><br>
>><br>
> _______________________________________________<br>
> Ifeffit mailing list<br>
> <a href="mailto:Ifeffit@millenia.cars.aps.anl.gov">Ifeffit@millenia.cars.aps.anl.gov</a><br>
> <a href="http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit" rel="noreferrer" target="_blank">http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit</a><br>
> Unsubscribe: <a href="http://millenia.cars.aps.anl.gov/mailman/options/ifeffit" rel="noreferrer" target="_blank">http://millenia.cars.aps.anl.gov/mailman/options/ifeffit</a><br>
><br>
><br>
><br>
> _______________________________________________<br>
> Ifeffit mailing list<br>
> <a href="mailto:Ifeffit@millenia.cars.aps.anl.gov">Ifeffit@millenia.cars.aps.anl.gov</a><br>
> <a href="http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit" rel="noreferrer" target="_blank">http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit</a><br>
> Unsubscribe: <a href="http://millenia.cars.aps.anl.gov/mailman/options/ifeffit" rel="noreferrer" target="_blank">http://millenia.cars.aps.anl.gov/mailman/options/ifeffit</a><br>
><br>
><br>
-------------- next part --------------<br>
An HTML attachment was scrubbed...<br>
URL: <<a href="http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20160623/e80e582d/attachment.html" rel="noreferrer" target="_blank">http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20160623/e80e582d/attachment.html</a>><br>
<br>
------------------------------<br>
<br>
Subject: Digest Footer<br>
<br>
_______________________________________________<br>
Ifeffit mailing list<br>
<a href="mailto:Ifeffit@millenia.cars.aps.anl.gov">Ifeffit@millenia.cars.aps.anl.gov</a><br>
<a href="http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit" rel="noreferrer" target="_blank">http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit</a><br>
Unsubscribe: <a href="http://millenia.cars.aps.anl.gov/mailman/options/ifeffit" rel="noreferrer" target="_blank">http://millenia.cars.aps.anl.gov/mailman/options/ifeffit</a><br>
<br>
<br>
------------------------------<br>
<br>
End of Ifeffit Digest, Vol 160, Issue 17<br>
****************************************<br>
</blockquote></div>