<div style="direction:ltr; font-family:Tahoma; color:#000000; font-size:10pt">Dear Anatoly,<br>
<br>
thanks a lot for your reply!<br>
I don't see the problem yet. In the attached file ("different_Au_foils.prj), there are two different gold reference foils measured at two different synchrotrons. There is some difference but not realy much. Could you please describe the regions that are worse
 comparing my gold foil-file to yours, or if possible, attache the file with both foils or at least a screenshot of the plot?<br>
<br>
Best regards,<br>
Julian<br>
<br>
<br>
<br>
<div style="font-family:Times New Roman; color:rgb(0,0,0); font-size:16px">
<hr tabindex="-1">
<div id="divRpF803870" style="direction:ltr"><font color="#000000" face="Tahoma" size="2"><b>Von:</b> ifeffit-bounces@millenia.cars.aps.anl.gov [ifeffit-bounces@millenia.cars.aps.anl.gov]" im Auftrag von "Anatoly I Frenkel [afrenke2@yu.edu]<br>
<b>Gesendet:</b> Dienstag, 11. Oktober 2011 20:29<br>
<b>Bis:</b> XAFS Analysis using Ifeffit<br>
<b>Betreff:</b> Re: [Ifeffit] Gold Nanoparticle first shell fitting<br>
</font><br>
</div>
<div>
<div style="direction:ltr; font-family:Tahoma; color:rgb(0,0,0); font-size:10pt">
<p>Something is horribly wrong with the data here.</p>
<p>I overplotted your reference Au foil against mine, and yours has distorted XANES and too high EXAFS intensity compared to my data. Your amplitude factor is 1.54 which also confirms that something was wrong in the experiment. Perhaps - a misalignment? The
 NP data also look strange... </p>
<p>I would not focus on the NP analysis until you figure out why your foil data is so strange.</p>
<p> </p>
<div>
<p> </p>
<div style="font-family:Tahoma; font-size:13px">
<div dir="ltr" id="idSignature25561">
<hr tabindex="-1">
</div>
</div>
</div>
<div style="font-family:Times New Roman; color:rgb(0,0,0); font-size:16px">
<div id="divRpF134176" style="direction:ltr"><font color="#000000" face="Tahoma" size="2"><b>From:</b> ifeffit-bounces@millenia.cars.aps.anl.gov [ifeffit-bounces@millenia.cars.aps.anl.gov] on behalf of Kaiser, Julian [julian.kaiser@helmholtz-berlin.de]<br>
<b>Sent:</b> Tuesday, October 11, 2011 1:06 PM<br>
<b>To:</b> ifeffit@millenia.cars.aps.anl.gov<br>
<b>Subject:</b> [Ifeffit] Gold Nanoparticle first shell fitting<br>
</font><br>
</div>
<div></div>
<div>
<div style="font-family:Tahoma; direction:ltr; color:rgb(0,0,0); font-size:10pt">
<span style="background-color:white"><span lang="en-US"><font face="Calibri,sans-serif" size="2"><span style="font-size:11pt"><span lang="de">Dear Ifeffit Community,<br>
<br>
I'm trying to fit a gold nanoparticle in the size of about 2 nm that is immobilized by polymers. For my research it's enought to fit the first shell only, becaues all I would like to analyze is the atomic distance in the nanoparticle. After the (hopefully)
 correct background substraction in Athena (athena file attached), there is a shoulder at approx. 2.1 Angström in the R-space.
<br>
In Artemis, fitting this shoulder seems not to be possible, while the fit for the reference (gold foil) seems to be fine. (both artemis files are attached to the e-mail).<br>
If the k-range is decreased from 12.388 to a value between 9 an 10, the shoulder disappears and the fit works fine. But I think by this change I might modify the data too much.<br>
Would be really nice, if sombody has an idea how to deal with the problem, to get a hint how to solve this.<br>
<br>
Thanks a lot,<br>
Julian</span></span></font></span></span></div>
<br>
<hr>
<font color="gray" face="Arial" size="1"><br>
Helmholtz-Zentrum Berlin für Materialien und Energie GmbH<br>
<br>
Mitglied der Hermann von Helmholtz-Gemeinschaft Deutscher Forschungszentren e.V.<br>
<br>
Aufsichtsrat: Vorsitzender Prof. Dr. Dr. h.c. mult. Joachim Treusch, stv. Vorsitzende Dr. Beatrix Vierkorn-Rudolph<br>
Geschäftsführer: Prof. Dr. Anke Rita Kaysser-Pyzalla, Dr. Ulrich Breuer<br>
<br>
Sitz Berlin, AG Charlottenburg, 89 HRB 5583<br>
<br>
Postadresse:<br>
Hahn-Meitner-Platz 1<br>
D-14109 Berlin<br>
<br>
http://www.helmholtz-berlin.de<br>
</font></div>
</div>
</div>
</div>
</div>
</div>
<br>
<hr>
<font face="Arial" color="Gray" size="1"><br>
Helmholtz-Zentrum Berlin für Materialien und Energie GmbH<br>
<br>
Mitglied der Hermann von Helmholtz-Gemeinschaft Deutscher Forschungszentren e.V.<br>
<br>
Aufsichtsrat: Vorsitzender Prof. Dr. Dr. h.c. mult. Joachim Treusch, stv. Vorsitzende Dr. Beatrix Vierkorn-Rudolph<br>
Geschäftsführer: Prof. Dr. Anke Rita Kaysser-Pyzalla, Dr. Ulrich Breuer<br>
<br>
Sitz Berlin, AG Charlottenburg, 89 HRB 5583<br>
<br>
Postadresse:<br>
Hahn-Meitner-Platz 1<br>
D-14109 Berlin<br>
<br>
http://www.helmholtz-berlin.de<br>
</font>
</body>
</html>