[Ifeffit] Fe K-edge maghemite (gamma-Fe2O3)
Christian Wittee Lopes
chriswittee at gmail.com
Sat Feb 17 10:28:56 CST 2024
Dear XAFS community,
I wonder if anyone has a CuSiO3 spectrum measured at Cu K-edge?
Thank you, again!
Em sex., 9 de fev. de 2024 às 05:58, Morgane Desmau <
morgane.desmau at gmail.com> escreveu:
> Hi,
>
> I have some but for nanoparticles maghemite (room temperature and 20K,
> continuous scanning mode).
>
> Best,
> Morgane Desmau
>
> Le jeu. 8 févr. 2024, à 13 h 11, Christian Wittee Lopes <
> chriswittee at gmail.com> a écrit :
>
>> Dear XAFS community,
>>
>> Does anyone have a Fe K-edge XAS spectrum of maghemite (gamma-Fe2O3)
>> sample or standard?
>>
>> Thank you in advance.
>>
>> Best,
>>
>> Christian Wittee Lopes
>>
>> --
>>
>> Christian Wittee Lopes
>>
>> Professor Adjunto
>>
>> *Departamento de Química - Setor de Ciências Exatas*
>>
>> Universidade Federal do Paraná (UFPR)
>>
>> *Curitiba - Paraná*
>>
>> *LinkedIn <https://urldefense.us/v3/__https://www.linkedin.com/in/christian-wittee-lopes-561855219/__;!!G_uCfscf7eWS!eFcwWUu4VfNRwi1wTzYci8AJYPyrJYLXh7duGqtivxZv1AE5mPoYiXb1ENtYktsPKLMGbv5u888KMTqMfkK2xOaYxqAOhHj9aw$ >
>> | ORCID <https://urldefense.us/v3/__https://orcid.org/my-orcid?orcid=0000-0001-8420-1958__;!!G_uCfscf7eWS!eFcwWUu4VfNRwi1wTzYci8AJYPyrJYLXh7duGqtivxZv1AE5mPoYiXb1ENtYktsPKLMGbv5u888KMTqMfkK2xOaYxqBwDSzRLg$ > | Lattes
>> <https://urldefense.us/v3/__http://lattes.cnpq.br/4953371870936050__;!!G_uCfscf7eWS!eFcwWUu4VfNRwi1wTzYci8AJYPyrJYLXh7duGqtivxZv1AE5mPoYiXb1ENtYktsPKLMGbv5u888KMTqMfkK2xOaYxqAy7MN43w$ >*
>> _______________________________________________
>> Ifeffit mailing list
>> Ifeffit at millenia.cars.aps.anl.gov
>> https://urldefense.us/v3/__http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit__;!!G_uCfscf7eWS!eFcwWUu4VfNRwi1wTzYci8AJYPyrJYLXh7duGqtivxZv1AE5mPoYiXb1ENtYktsPKLMGbv5u888KMTqMfkK2xOaYxqBqZw1wkg$
>> Unsubscribe: https://urldefense.us/v3/__http://millenia.cars.aps.anl.gov/mailman/options/ifeffit__;!!G_uCfscf7eWS!eFcwWUu4VfNRwi1wTzYci8AJYPyrJYLXh7duGqtivxZv1AE5mPoYiXb1ENtYktsPKLMGbv5u888KMTqMfkK2xOaYxqAqjmdJBg$
>>
> _______________________________________________
> Ifeffit mailing list
> Ifeffit at millenia.cars.aps.anl.gov
> https://urldefense.us/v3/__http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit__;!!G_uCfscf7eWS!eFcwWUu4VfNRwi1wTzYci8AJYPyrJYLXh7duGqtivxZv1AE5mPoYiXb1ENtYktsPKLMGbv5u888KMTqMfkK2xOaYxqBqZw1wkg$
> Unsubscribe: https://urldefense.us/v3/__http://millenia.cars.aps.anl.gov/mailman/options/ifeffit__;!!G_uCfscf7eWS!eFcwWUu4VfNRwi1wTzYci8AJYPyrJYLXh7duGqtivxZv1AE5mPoYiXb1ENtYktsPKLMGbv5u888KMTqMfkK2xOaYxqAqjmdJBg$
>
--
Christian Wittee Lopes
Professor Adjunto
*Departamento de Química - Setor de Ciências Exatas*
Universidade Federal do Paraná (UFPR)
*Curitiba - Paraná*
*LinkedIn <https://urldefense.us/v3/__https://www.linkedin.com/in/christian-wittee-lopes-561855219/__;!!G_uCfscf7eWS!eFcwWUu4VfNRwi1wTzYci8AJYPyrJYLXh7duGqtivxZv1AE5mPoYiXb1ENtYktsPKLMGbv5u888KMTqMfkK2xOaYxqAOhHj9aw$ > |
ORCID <https://urldefense.us/v3/__https://orcid.org/my-orcid?orcid=0000-0001-8420-1958__;!!G_uCfscf7eWS!eFcwWUu4VfNRwi1wTzYci8AJYPyrJYLXh7duGqtivxZv1AE5mPoYiXb1ENtYktsPKLMGbv5u888KMTqMfkK2xOaYxqBwDSzRLg$ > | Lattes
<https://urldefense.us/v3/__http://lattes.cnpq.br/4953371870936050__;!!G_uCfscf7eWS!eFcwWUu4VfNRwi1wTzYci8AJYPyrJYLXh7duGqtivxZv1AE5mPoYiXb1ENtYktsPKLMGbv5u888KMTqMfkK2xOaYxqAy7MN43w$ >*
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20240217/41963719/attachment.htm>
More information about the Ifeffit
mailing list