[Ifeffit] [Ext] Zr K edge EXAFS analysis of amorphous materials
Angshuman Gupta
angshumanmet at gmail.com
Sat Feb 11 23:27:46 CST 2023
Dear Prof. Carlo Segre,
Thank you for your reply. I have attached the Athena file with Zr foil as
reference.
Thank you
Angshuman Gupta
PhD research scholar
Department of Metallurgical Engineering and Materials science.
Indian Institute of Technology Bombay, Mumbai, India
On Sun, Feb 12, 2023 at 6:56 AM Carlo Segre <segre at iit.edu> wrote:
> Hi Angshuman:
>
> My advice is to go back to the background subtraction and adjust that
> first. You should be able to eliminate the peak below 1A and that might
> well affect the part of the data you are interested in. If you want to
> share the Athena project, I could give you more concrete advice.
>
> Carlo
>
> On Fri, Feb 10, 2023 at 2:35 AM Angshuman Gupta <angshumanmet at gmail.com>
> wrote:
>
>> Dear everyone,
>> I am working on alumina based amorphous materials containing ZrO2. I am
>> interested in finding the bond length between Zr and O atoms and
>> coordination number (N). Zr K edge spectra were collected at room
>> temperature at 300K along with Zr foil as reference. Extracted So2 from
>> reference (Zr foil) spectra was used to find N in the amorphous material.
>> Local environment around Zr was modelled with harmonic and quasi harmonic
>> models using a third cumulant of the distributions. Theoretical spectra fit
>> well using quasi-harmonic models with large bond length (2.21 A) while
>> harmonic models without third cumulants do not fit the spectra properly and
>> calculating higher N value with 2.16 A as Zr-O bond length.
>> I will be thankful if you kindly let me know what else we can do to
>> improve the fitting and get some meaningful outcome. Any relevant journal
>> articles are also helpful.
>> I have attached the Artemis files.
>>
>> Thanking you
>> Angshuman Gupta
>> PhD research scholar
>> IIT Bombay, Mumbai
>> _______________________________________________
>> Ifeffit mailing list
>> Ifeffit at millenia.cars.aps.anl.gov
>> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
>> Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit
>>
>
>
> --
> Carlo U. Segre (he/him) -- Duchossois Leadership Professor of Physics
> Professor of Materials Science & Engineering
> Director, Center for Synchrotron Radiation Research and Instrumentation
> Illinois Institute of Technology
> Voice: 312.567.3498 Fax: 312.567.3494
> segre at iit.edu http://phys.iit.edu/~segre segre at debian.org
>
> _______________________________________________
> Ifeffit mailing list
> Ifeffit at millenia.cars.aps.anl.gov
> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
> Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20230212/ce65a5c5/attachment-0001.htm>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: Zr edge AYZ RFF.prj
Type: application/octet-stream
Size: 17284 bytes
Desc: not available
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20230212/ce65a5c5/attachment-0002.obj>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: Zr reference RFF.prj
Type: application/octet-stream
Size: 26120 bytes
Desc: not available
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20230212/ce65a5c5/attachment-0003.obj>
More information about the Ifeffit
mailing list