[Ifeffit] Co2P spectrum
Yuji Hiraoka
hiraokay at spring8.or.jp
Mon Sep 12 19:02:27 CDT 2022
Dear Lopes,
You can download Co2P spectrum from following URL.
By using Si(311) plane as a monochromator:
https://mdr.nims.go.jp/concern/datasets/8336h411j?locale=en
By using Si(111) plane as a monochromator:
https://mdr.nims.go.jp/concern/datasets/p2676x842?locale=en
These data is originally uploaded at https://benten.spring8.or.jp/ , and
provided to above databases. If you have a interest, see this also.
Sincerely,
Yuji Hiraoka
>Dear XAFS community,
>
>Does anyone have a spectrum of Co2P sample or standard?
>
>Thank you in advance.
>
>Best,
>
>Christian Wittee Lopes
>
>--
>
>Christian Wittee Lopes
>
>Visiting Researcher - ANP/FINEP - PRH 50.1
>
>Institute of Chemistry, Universidade Federal do Rio Grande do Sul (UFRGS)
>
>chriswittee at gmail.com
>
>LinkedIn <https://www.linkedin.com/in/christian-wittee-lopes-561855219/> |
>ORCID <https://orcid.org/my-orcid?orcid=0000-0001-8420-1958> | Lattes
><http://lattes.cnpq.br/4953371870936050>
>
>
>--------html-part included links-------
>mailto:chriswittee at gmail.com
>
>-------------------------------text/plain-------------------------------
>_______________________________________________
>Ifeffit mailing list
>Ifeffit at millenia.cars.aps.anl.gov
>http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
>Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit
More information about the Ifeffit
mailing list