[Ifeffit] EXAFS Fitting with 2 CIF files
Kelly, Shelly D.
skelly at anl.gov
Tue Sep 7 10:00:56 CDT 2021
Hi Zihao:
Here is an artemis project file showing how I’d set this up. I put Pt foil data in it, since I don’t have your data.
Kind regards,
Shelly
From: Ifeffit <ifeffit-bounces at millenia.cars.aps.anl.gov> On Behalf Of Zihao Yan
Sent: Sunday, September 5, 2021 9:35 PM
To: XAFS Analysis using Ifeffit <ifeffit at millenia.cars.aps.anl.gov>
Subject: Re: [Ifeffit] EXAFS Fitting with 2 CIF files
Dear Scott, Matthew and Peng:
Thank you so much for your answers!
I have a couple of follow up questions:
1) for the CIF(Pt3Fe), there are 2 paths (Pt-Pt and Pt-Fe). Do the 2 paths share the same amplitude as: S02 * (1-fracoxide) ?
I attached screenshots of my settings. Could you please take a look?
2) Is there any way to set up constraints on Artemis? For example, I want to set 0<fracoxide<1. Sometimes, I got weird values of fracoxide, even with abs()
Thank you again for your help!
Sincerely,
Zihao Yan
On Sun, Sep 5, 2021 at 4:08 AM Peng Liu <liupeng5182 at gmail.com<mailto:liupeng5182 at gmail.com>> wrote:
Just a quick question. For Zihao' sample, the 1st peak for Pt-O from PtO2 is at 2.07 A and the 2nd peak for Pt-Pt or Pt-Fe from Pt3-Fe is at 2.736 A.
If these peaks are at different positions, could we use the molar ratio method to distinguish the contribution from each reference?
My understanding is that if two paths contribute to the same peak, then the molar ratio method can be applied.
I am not sure if my understanding is right or not.
Best Regards,
Peng Liu
China University of Geosciences
On Sun, Sep 5, 2021 at 5:00 AM Matthew Marcus <mamarcus at lbl.gov<mailto:mamarcus at lbl.gov>> wrote:
Extending what Scott said, I find it useful to make the coefficients
abs(fracoxide) and abs(1-abs(fracoxide)) to avoid false minima with
negative S0^2.
mam
On 9/4/2021 1:21 PM, Scott Calvin wrote:
> Hi Zihao,
>
> Do it by folding the molar ratio in to the amp parameter for each CIF. Of course S02 is part of that parameter, too.
>
> So the amp for PtO2 might be parameterized as S02 * fracoxide and the amp for Pt3Fe as S02 * (1-fracoxide)
>
> You could either assume the S02 is the same for the two phases (as I implicitly did by writing it with only one S02 variable), or you could use a standard for each (from a sample prepared and measured in a similar way) to fix the S02 for each phase.
>
> Best,
> Scott Calvin
> Lehman College of the City University of New York
>
>> On Sep 4, 2021, at 4:02 PM, Zihao Yan <zihao.yan.sci at gmail.com<mailto:zihao.yan.sci at gmail.com>> wrote:
>>
>> Dear Ifeffit members:
>>
>> I have a sample which is a mixture of PtFe and PtO2. In order to do the EXAFS fitting, I imported 2 CIF files on Artemis and generated the following 3 paths:
>> From PtO2: Pt-O @ 2.07 nm
>> From Pt3Fe: Pt-Pt @ 2.736 nm, Pt-Fe @ 2.736 nm
>> Then, I used these 3 bonds to do the fitting as in the online tutorial (which used 1 CIF file). The fitting result is good in terms of R^2 but it is not scientifically correct.
>>
>> I think I didn't set up a parameter which determines the ratio between CIF(PtO2) and CIF(Pt3Fe). I mean there should be a parameter that regulates how much each CIF contributes to the fitting or the molar ratio between PtO2 and Pt3Fe in my system.
>>
>> Could someone please give me some suggestions on how to do EXAFS fitting with 2 CIF files? Is there anywhere I can set up the molar ratio between PtO2 and Pt3Fe?
>>
>> Yours sincerely,
>> Zihao Yan
>> _______________________________________________
>> Ifeffit mailing list
>> Ifeffit at millenia.cars.aps.anl.gov<mailto:Ifeffit at millenia.cars.aps.anl.gov>
>> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
>> Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit
>
>
> _______________________________________________
> Ifeffit mailing list
> Ifeffit at millenia.cars.aps.anl.gov<mailto:Ifeffit at millenia.cars.aps.anl.gov>
> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
> Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit
>
_______________________________________________
Ifeffit mailing list
Ifeffit at millenia.cars.aps.anl.gov<mailto:Ifeffit at millenia.cars.aps.anl.gov>
http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit
--
Best Regards,
Peng Liu
_______________________________________________
Ifeffit mailing list
Ifeffit at millenia.cars.aps.anl.gov<mailto:Ifeffit at millenia.cars.aps.anl.gov>
http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20210907/b985001c/attachment-0001.htm>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: PtO2_Fe3Pt.fpj
Type: application/octet-stream
Size: 359812 bytes
Desc: PtO2_Fe3Pt.fpj
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20210907/b985001c/attachment-0001.obj>