[Ifeffit] Nanocrystalline NiO
Matthew Marcus
mamarcus at lbl.gov
Mon Jan 18 16:20:50 CST 2021
I have a spectrum which really belongs to Jordi Cabana and Ulrike Boesenberg and which were used in the attached paper.
Please get permission from one of these people before using it. The 'pristine' is bulk.
Sincerely,
Matthew Marcus
On 1/18/2021 2:07 PM, Christian Wittee Lopes wrote:
> Dear all,
>
> Firstly I would like to wish you a much better year than in 2020.
>
> Does anyone have some spectra of nanocrystalline NiO (not bulk standards)? I have a spectrum of a mixed compound and would like to get more insights into what I really have in this sample.
>
> Thank you in advance!!!
>
> Kind regards,
>
>
> --
> *Christian Wittee Lopes*
> /
> /
> /Visiting Researcher/
> ANP/FINEP - PRH50
> Institute of Chemistry, Universidade Federal do Rio Grande do Sul (UFRGS)
> Phone: +55 54 992430264
>
> _______________________________________________
> Ifeffit mailing list
> Ifeffit at millenia.cars.aps.anl.gov
> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
> Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit
>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: srep07133 (1).pdf
Type: application/pdf
Size: 1687349 bytes
Desc: not available
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20210118/6de28b2f/attachment-0001.pdf>
-------------- next part --------------
8.2316064E+3 1.2460149E-3
8.2366065E+3 1.4793792E-3
8.2416067E+3 1.6763827E-3
8.2466068E+3 1.6317915E-3
8.2516070E+3 1.7582957E-3
8.2566071E+3 1.6515803E-3
8.2616072E+3 2.0952501E-3
8.2666074E+3 2.1554625E-3
8.2716075E+3 2.3964267E-3
8.2766077E+3 2.7184428E-3
8.2816078E+3 2.9151296E-3
8.2866080E+3 3.3403745E-3
8.2916081E+3 4.0589194E-3
8.2966083E+3 3.4122299E-3
8.3016084E+3 4.1509290E-3
8.3066086E+3 5.5472506E-3
8.3116087E+3 7.0882989E-3
8.3121087E+3 6.7281363E-3
8.3126087E+3 6.6862830E-3
8.3131088E+3 6.7701557E-3
8.3136088E+3 6.9752720E-3
8.3141088E+3 7.0065226E-3
8.3146088E+3 7.4805818E-3
8.3151088E+3 8.5669886E-3
8.3156088E+3 8.3118100E-3
8.3161088E+3 7.9527824E-3
8.3166089E+3 7.9749572E-3
8.3171089E+3 8.2385041E-3
8.3176089E+3 8.2735361E-3
8.3181089E+3 8.7199093E-3
8.3186089E+3 9.1019289E-3
8.3191089E+3 9.1394568E-3
8.3196089E+3 9.5330423E-3
8.3201090E+3 9.7359248E-3
8.3206090E+3 1.0404152E-2
8.3211090E+3 1.1121663E-2
8.3216090E+3 1.1528490E-2
8.3221090E+3 1.1827616E-2
8.3226090E+3 1.2199642E-2
8.3231091E+3 1.2195658E-2
8.3236091E+3 1.3237446E-2
8.3241091E+3 1.3889887E-2
8.3246091E+3 1.5159374E-2
8.3251091E+3 1.5539870E-2
8.3256091E+3 1.6185819E-2
8.3261091E+3 1.6793515E-2
8.3266092E+3 1.7458003E-2
8.3271092E+3 1.8565124E-2
8.3276092E+3 1.9882821E-2
8.3281092E+3 2.1187953E-2
8.3286092E+3 2.1955502E-2
8.3291092E+3 2.3820709E-2
8.3296092E+3 2.6436867E-2
8.3301093E+3 2.9557773E-2
8.3306093E+3 3.4992527E-2
8.3311093E+3 4.2085814E-2
8.3316093E+3 4.8755423E-2
8.3321093E+3 4.9709093E-2
8.3326093E+3 4.7157604E-2
8.3331093E+3 4.6339530E-2
8.3336094E+3 4.8267792E-2
8.3341094E+3 5.2632993E-2
8.3346094E+3 5.9288549E-2
8.3351094E+3 6.9084534E-2
8.3356094E+3 8.2138766E-2
8.3361094E+3 9.5573015E-2
8.3366094E+3 1.0957398E-1
8.3371095E+3 1.2839516E-1
8.3376095E+3 1.4950528E-1
8.3381095E+3 1.8353240E-1
8.3386095E+3 2.2706347E-1
8.3391095E+3 2.7861999E-1
8.3396095E+3 3.3649083E-1
8.3401096E+3 3.8670135E-1
8.3406096E+3 4.3216611E-1
8.3411096E+3 4.8959628E-1
8.3416096E+3 5.4482993E-1
8.3421096E+3 6.1294780E-1
8.3426096E+3 6.8024796E-1
8.3431096E+3 7.6596771E-1
8.3436097E+3 8.7743535E-1
8.3441097E+3 9.8031974E-1
8.3446097E+3 1.0937161E+0
8.3451097E+3 1.1757946E+0
8.3456097E+3 1.2449745E+0
8.3461097E+3 1.3160904E+0
8.3466097E+3 1.3756815E+0
8.3471098E+3 1.4378302E+0
8.3476098E+3 1.5131641E+0
8.3481098E+3 1.5747498E+0
8.3486098E+3 1.6168092E+0
8.3491098E+3 1.6225129E+0
8.3496098E+3 1.6035003E+0
8.3501098E+3 1.5543196E+0
8.3506099E+3 1.4924833E+0
8.3511099E+3 1.4268707E+0
8.3516099E+3 1.3496396E+0
8.3521099E+3 1.2906728E+0
8.3526099E+3 1.2370054E+0
8.3531099E+3 1.1861179E+0
8.3536100E+3 1.1456613E+0
8.3541100E+3 1.1131266E+0
8.3546100E+3 1.0826292E+0
8.3551100E+3 1.0525643E+0
8.3556100E+3 1.0176343E+0
8.3561100E+3 9.8303504E-1
8.3566100E+3 9.4283622E-1
8.3571101E+3 9.0434480E-1
8.3576101E+3 8.7615715E-1
8.3581101E+3 8.5277118E-1
8.3586101E+3 8.3171509E-1
8.3591101E+3 8.1806563E-1
8.3596101E+3 8.0952729E-1
8.3601101E+3 8.0696072E-1
8.3606102E+3 8.1098476E-1
8.3611102E+3 8.1923333E-1
8.3616102E+3 8.3499585E-1
8.3636144E+3 9.1181020E-1
8.3656186E+3 9.3129595E-1
8.3676228E+3 8.9581575E-1
8.3696270E+3 8.6202100E-1
8.3716311E+3 8.3400214E-1
8.3736353E+3 8.0910329E-1
8.3756395E+3 7.9941294E-1
8.3776437E+3 8.1540374E-1
8.3796479E+3 8.4713954E-1
8.3816521E+3 8.8040787E-1
8.3836563E+3 9.0571371E-1
8.3856605E+3 9.3467944E-1
8.3876647E+3 9.7918478E-1
8.3896689E+3 1.0318247E+0
8.3916731E+3 1.0813841E+0
8.3936773E+3 1.1165049E+0
8.3956814E+3 1.1385288E+0
8.3976856E+3 1.1511347E+0
8.3996898E+3 1.1451416E+0
8.4016940E+3 1.1216301E+0
8.4036982E+3 1.0889921E+0
8.4057024E+3 1.0518465E+0
8.4077066E+3 1.0182888E+0
8.4097108E+3 9.8612572E-1
8.4117150E+3 9.5856413E-1
8.4137192E+3 9.3566774E-1
8.4157234E+3 9.1793551E-1
8.4177276E+3 9.0842961E-1
8.4197317E+3 9.0696703E-1
8.4217359E+3 9.1201954E-1
8.4237401E+3 9.2302266E-1
8.4257443E+3 9.3672374E-1
8.4277485E+3 9.4999103E-1
8.4297527E+3 9.5736984E-1
8.4317569E+3 9.6182422E-1
8.4337611E+3 9.6469121E-1
8.4357653E+3 9.6958905E-1
8.4377695E+3 9.7594345E-1
8.4397737E+3 9.8577045E-1
8.4417779E+3 9.9989791E-1
8.4437821E+3 1.0155560E+0
8.4457862E+3 1.0278709E+0
8.4477904E+3 1.0329944E+0
8.4497946E+3 1.0302152E+0
8.4520558E+3 1.0194594E+0
8.4543169E+3 1.0022746E+0
8.4565780E+3 9.8390803E-1
8.4588392E+3 9.6293263E-1
8.4611003E+3 9.4523433E-1
8.4633615E+3 9.3453140E-1
8.4656226E+3 9.3582555E-1
8.4678837E+3 9.4989428E-1
8.4701449E+3 9.7231235E-1
8.4724060E+3 9.9935940E-1
8.4746672E+3 1.0201046E+0
8.4769283E+3 1.0327100E+0
8.4791894E+3 1.0343250E+0
8.4814506E+3 1.0292013E+0
8.4837117E+3 1.0204819E+0
8.4859729E+3 1.0144707E+0
8.4882340E+3 1.0153284E+0
8.4904952E+3 1.0196892E+0
8.4927563E+3 1.0264258E+0
8.4950174E+3 1.0342815E+0
8.4972786E+3 1.0403690E+0
8.4995397E+3 1.0430828E+0
8.5018009E+3 1.0426297E+0
8.5040620E+3 1.0384375E+0
8.5063231E+3 1.0313037E+0
8.5085843E+3 1.0194884E+0
8.5108454E+3 1.0060790E+0
8.5131066E+3 9.9041690E-1
8.5153677E+3 9.7306642E-1
8.5176288E+3 9.5668750E-1
8.5198900E+3 9.4141100E-1
8.5221511E+3 9.2987528E-1
8.5244123E+3 9.2354597E-1
8.5266734E+3 9.2307026E-1
8.5289345E+3 9.3047381E-1
8.5311957E+3 9.4315648E-1
8.5334568E+3 9.6013024E-1
8.5357180E+3 9.7812615E-1
8.5379791E+3 9.9483888E-1
8.5404987E+3 1.0110561E+0
8.5430182E+3 1.0224487E+0
8.5455378E+3 1.0307371E+0
8.5480573E+3 1.0340081E+0
8.5505769E+3 1.0344115E+0
8.5530964E+3 1.0331541E+0
8.5556160E+3 1.0300672E+0
8.5581356E+3 1.0259220E+0
8.5606551E+3 1.0217437E+0
8.5631747E+3 1.0185599E+0
8.5656942E+3 1.0151457E+0
8.5682138E+3 1.0125115E+0
8.5707333E+3 1.0105728E+0
8.5732529E+3 1.0071155E+0
8.5757725E+3 1.0033821E+0
8.5782920E+3 1.0006339E+0
8.5808116E+3 9.9832820E-1
8.5833311E+3 9.9679062E-1
8.5858507E+3 9.9714413E-1
8.5883702E+3 9.9684617E-1
8.5908898E+3 9.9676189E-1
8.5934094E+3 9.9485380E-1
8.5959289E+3 9.9217873E-1
8.5984485E+3 9.8766356E-1
8.6009680E+3 9.8346472E-1
8.6034876E+3 9.8061687E-1
8.6060071E+3 9.7964311E-1
8.6085267E+3 9.7923731E-1
8.6110463E+3 9.8062782E-1
8.6135658E+3 9.8367080E-1
8.6160854E+3 9.8885792E-1
8.6186049E+3 9.9251778E-1
8.6211245E+3 9.9541023E-1
8.6236440E+3 1.0008445E+0
8.6261636E+3 1.0053323E+0
8.6290083E+3 1.0108198E+0
8.6318529E+3 1.0152371E+0
8.6346976E+3 1.0168119E+0
8.6375422E+3 1.0173977E+0
8.6403869E+3 1.0177455E+0
8.6432316E+3 1.0154347E+0
8.6460762E+3 1.0135769E+0
8.6489209E+3 1.0085603E+0
8.6517656E+3 1.0020884E+0
8.6546102E+3 9.9620968E-1
8.6574549E+3 9.9092214E-1
8.6602995E+3 9.8715195E-1
8.6631442E+3 9.8437928E-1
8.6659889E+3 9.8490380E-1
8.6688335E+3 9.8651367E-1
8.6716782E+3 9.8801610E-1
8.6745228E+3 9.8921549E-1
8.6773675E+3 9.9023489E-1
8.6802122E+3 9.9124598E-1
8.6830568E+3 9.9058247E-1
8.6859015E+3 9.9043213E-1
8.6887462E+3 9.9069630E-1
8.6915908E+3 9.9375980E-1
8.6944355E+3 9.9617939E-1
8.6972801E+3 9.9954656E-1
8.7001248E+3 1.0032708E+0
8.7029695E+3 1.0063592E+0
8.7058141E+3 1.0099597E+0
8.7086588E+3 1.0123900E+0
8.7115035E+3 1.0147777E+0
8.7143481E+3 1.0160414E+0
8.7173890E+3 1.0157375E+0
8.7204298E+3 1.0143761E+0
8.7234707E+3 1.0117998E+0
8.7265115E+3 1.0089594E+0
8.7295524E+3 1.0057434E+0
8.7325932E+3 1.0006195E+0
8.7356340E+3 9.9649888E-1
8.7386749E+3 9.9217778E-1
8.7417157E+3 9.8912265E-1
8.7447566E+3 9.8739565E-1
8.7477974E+3 9.8762911E-1
8.7508383E+3 9.8880623E-1
8.7538791E+3 9.9066705E-1
8.7569200E+3 9.9334953E-1
8.7599608E+3 9.9551743E-1
8.7630017E+3 9.9664035E-1
8.7660425E+3 9.9716375E-1
8.7690834E+3 9.9727026E-1
8.7721242E+3 9.9774591E-1
8.7751651E+3 9.9769279E-1
8.7782059E+3 9.9804948E-1
8.7812467E+3 9.9773316E-1
8.7842876E+3 9.9701346E-1
8.7873284E+3 9.9802731E-1
8.7903693E+3 9.9940054E-1
8.7934101E+3 1.0002061E+0
8.7964510E+3 1.0011316E+0
8.7994918E+3 1.0027635E+0
8.8025327E+3 1.0039248E+0
8.8059244E+3 1.0048820E+0
8.8093161E+3 1.0069235E+0
8.8127078E+3 1.0091062E+0
8.8160995E+3 1.0107551E+0
8.8194912E+3 1.0106834E+0
8.8228830E+3 1.0105649E+0
8.8262747E+3 1.0096880E+0
8.8296664E+3 1.0095806E+0
8.8330581E+3 1.0084990E+0
8.8364498E+3 1.0072841E+0
8.8398415E+3 1.0057034E+0
8.8432332E+3 1.0040360E+0
8.8466250E+3 1.0036670E+0
8.8500167E+3 1.0030774E+0
8.8534084E+3 1.0030081E+0
8.8568001E+3 1.0024990E+0
8.8601918E+3 1.0022452E+0
8.8635835E+3 1.0027207E+0
8.8669752E+3 1.0035254E+0
8.8703670E+3 1.0026064E+0
8.8737587E+3 1.0034891E+0
8.8771504E+3 1.0045430E+0
8.8805421E+3 1.0049623E+0
8.8839338E+3 1.0044841E+0
8.8873255E+3 1.0060078E+0
8.8907173E+3 1.0072633E+0
8.8943916E+3 1.0075458E+0
8.8980660E+3 1.0093169E+0
8.9017403E+3 1.0109209E+0
8.9054147E+3 1.0133200E+0
8.9090890E+3 1.0148400E+0
8.9127634E+3 1.0149890E+0
8.9164378E+3 1.0151294E+0
8.9201121E+3 1.0148043E+0
8.9237865E+3 1.0137022E+0
8.9274608E+3 1.0129851E+0
8.9311352E+3 1.0121241E+0
8.9348096E+3 1.0115116E+0
8.9384839E+3 1.0113599E+0
8.9421583E+3 1.0121646E+0
8.9458326E+3 1.0125751E+0
8.9495070E+3 1.0124518E+0
8.9531813E+3 1.0122118E+0
8.9568557E+3 1.0119550E+0
8.9605301E+3 1.0121961E+0
8.9642044E+3 1.0125556E+0
8.9678788E+3 1.0123913E+0
8.9715531E+3 1.0143750E+0
8.9752275E+3 1.0149052E+0
8.9789019E+3 1.0149266E+0
8.9827360E+3 1.0163669E+0
8.9865701E+3 1.0168249E+0
8.9904042E+3 1.0178274E+0
8.9942383E+3 1.0181719E+0
8.9980724E+3 1.0195063E+0
9.0019065E+3 1.0208873E+0
9.0057407E+3 1.0215341E+0
9.0095748E+3 1.0220925E+0
9.0134089E+3 1.0229333E+0
9.0172430E+3 1.0238930E+0
9.0210771E+3 1.0241327E+0
9.0249112E+3 1.0241039E+0
9.0287453E+3 1.0238570E+0
9.0325795E+3 1.0232697E+0
9.0364136E+3 1.0238954E+0
9.0402477E+3 1.0243265E+0
9.0440818E+3 1.0232058E+0
9.0479159E+3 1.0240996E+0
9.0517500E+3 1.0241860E+0
9.0555841E+3 1.0243291E+0
9.0594183E+3 1.0254229E+0
9.0632524E+3 1.0260072E+0
-------------- next part --------------
8.2603600E+3 1.3614900E-3
8.2703600E+3 2.4961500E-3
8.2803600E+3 2.8457100E-3
8.2903600E+3 3.0380200E-3
8.3003600E+3 3.5157900E-3
8.3103600E+3 6.3899600E-3
8.3106100E+3 6.8502800E-3
8.3108600E+3 6.6812200E-3
8.3111100E+3 6.2742500E-3
8.3113600E+3 6.9301500E-3
8.3116100E+3 6.4737000E-3
8.3118600E+3 6.4662900E-3
8.3121100E+3 6.5408900E-3
8.3123600E+3 6.2317400E-3
8.3126100E+3 6.6055200E-3
8.3128600E+3 6.3178900E-3
8.3131100E+3 6.4576900E-3
8.3133600E+3 6.3840300E-3
8.3136100E+3 6.5933500E-3
8.3138600E+3 6.6391200E-3
8.3141100E+3 6.7374800E-3
8.3143600E+3 6.8033600E-3
8.3146100E+3 6.9112400E-3
8.3148600E+3 7.2876100E-3
8.3151100E+3 7.4669900E-3
8.3153600E+3 7.3732700E-3
8.3156100E+3 7.6880800E-3
8.3158600E+3 7.5832900E-3
8.3161100E+3 7.3999200E-3
8.3163600E+3 7.5337300E-3
8.3166100E+3 7.9496000E-3
8.3168600E+3 7.6249300E-3
8.3171100E+3 7.7581600E-3
8.3173600E+3 7.5351800E-3
8.3176100E+3 7.5308400E-3
8.3178600E+3 8.1140100E-3
8.3181100E+3 7.8568500E-3
8.3183600E+3 7.6679100E-3
8.3186100E+3 8.3204300E-3
8.3188600E+3 8.3745200E-3
8.3191100E+3 8.2452100E-3
8.3193600E+3 8.0714900E-3
8.3196100E+3 8.3526900E-3
8.3198600E+3 8.7463300E-3
8.3201100E+3 8.9480100E-3
8.3203600E+3 9.2352700E-3
8.3206100E+3 9.5853600E-3
8.3208600E+3 9.9916600E-3
8.3211100E+3 1.0621200E-2
8.3213600E+3 1.0774100E-2
8.3216100E+3 1.0897000E-2
8.3218600E+3 1.0873900E-2
8.3221100E+3 1.0698000E-2
8.3223600E+3 1.0725100E-2
8.3226100E+3 1.0452400E-2
8.3228600E+3 1.1256600E-2
8.3231100E+3 1.1575500E-2
8.3233600E+3 1.2732400E-2
8.3236100E+3 1.2704200E-2
8.3238600E+3 1.2795800E-2
8.3241100E+3 1.3090300E-2
8.3243600E+3 1.2983300E-2
8.3246100E+3 1.3172300E-2
8.3248600E+3 1.3582600E-2
8.3251100E+3 1.3869400E-2
8.3253600E+3 1.4079200E-2
8.3256100E+3 1.4477300E-2
8.3258600E+3 1.5013700E-2
8.3261100E+3 1.4997800E-2
8.3263600E+3 1.5176900E-2
8.3266100E+3 1.5390800E-2
8.3268600E+3 1.5837700E-2
8.3271100E+3 1.6114000E-2
8.3273700E+3 1.6530400E-2
8.3276100E+3 1.7426700E-2
8.3278600E+3 1.7922600E-2
8.3281100E+3 1.8412600E-2
8.3283600E+3 1.9311600E-2
8.3286100E+3 1.9665700E-2
8.3288600E+3 2.0272100E-2
8.3291100E+3 2.1055500E-2
8.3293600E+3 2.1974600E-2
8.3296100E+3 2.3106700E-2
8.3298600E+3 2.4160200E-2
8.3301100E+3 2.6233000E-2
8.3303600E+3 2.8990500E-2
8.3306100E+3 3.1799800E-2
8.3308600E+3 3.5647900E-2
8.3311100E+3 3.9786800E-2
8.3313600E+3 4.2873300E-2
8.3316100E+3 4.4070400E-2
8.3318600E+3 4.5287500E-2
8.3321100E+3 4.4655400E-2
8.3323600E+3 4.3685700E-2
8.3326100E+3 4.2377400E-2
8.3328600E+3 4.1288600E-2
8.3331100E+3 4.0778500E-2
8.3333600E+3 4.2076500E-2
8.3336100E+3 4.3163400E-2
8.3338600E+3 4.5030800E-2
8.3341100E+3 4.7715000E-2
8.3343600E+3 5.1042600E-2
8.3346100E+3 5.5646200E-2
8.3348600E+3 6.1659300E-2
8.3351100E+3 6.7562500E-2
8.3353600E+3 7.4087300E-2
8.3356100E+3 8.0457600E-2
8.3358600E+3 8.6985200E-2
8.3361100E+3 9.4160600E-2
8.3363600E+3 1.0051600E-1
8.3366100E+3 1.0819500E-1
8.3368600E+3 1.1642700E-1
8.3371100E+3 1.2561200E-1
8.3373600E+3 1.3691700E-1
8.3376100E+3 1.5025300E-1
8.3378600E+3 1.6573700E-1
8.3381100E+3 1.8480500E-1
8.3383600E+3 2.0779800E-1
8.3386100E+3 2.3355100E-1
8.3388600E+3 2.6085500E-1
8.3391100E+3 2.8921400E-1
8.3393600E+3 3.1711700E-1
8.3396100E+3 3.4535000E-1
8.3398600E+3 3.7188700E-1
8.3401100E+3 3.9759700E-1
8.3403600E+3 4.2458100E-1
8.3406100E+3 4.4953600E-1
8.3408600E+3 4.7456400E-1
8.3411100E+3 4.9948900E-1
8.3413600E+3 5.2547200E-1
8.3416100E+3 5.5097400E-1
8.3418600E+3 5.7778300E-1
8.3421100E+3 6.0755300E-1
8.3423600E+3 6.4085600E-1
8.3426100E+3 6.7921600E-1
8.3428600E+3 7.2316600E-1
8.3431100E+3 7.7213300E-1
8.3433600E+3 8.2598300E-1
8.3436100E+3 8.8206200E-1
8.3438600E+3 9.3753700E-1
8.3441100E+3 9.9098100E-1
8.3443600E+3 1.0388400E+0
8.3446100E+3 1.0813600E+0
8.3448600E+3 1.1203900E+0
8.3451100E+3 1.1551400E+0
8.3453600E+3 1.1886900E+0
8.3456100E+3 1.2203000E+0
8.3458600E+3 1.2518500E+0
8.3461100E+3 1.2831800E+0
8.3463600E+3 1.3161700E+0
8.3466100E+3 1.3517900E+0
8.3468600E+3 1.3889700E+0
8.3471100E+3 1.4290300E+0
8.3473600E+3 1.4699400E+0
8.3476100E+3 1.5109700E+0
8.3478600E+3 1.5495700E+0
8.3481100E+3 1.5820600E+0
8.3483600E+3 1.6068400E+0
8.3486100E+3 1.6213300E+0
8.3488600E+3 1.6267700E+0
8.3491100E+3 1.6211400E+0
8.3493600E+3 1.6083100E+0
8.3496100E+3 1.5869200E+0
8.3498600E+3 1.5602600E+0
8.3501100E+3 1.5294900E+0
8.3503600E+3 1.4963500E+0
8.3506100E+3 1.4623800E+0
8.3508600E+3 1.4257400E+0
8.3511100E+3 1.3894500E+0
8.3513600E+3 1.3543600E+0
8.3516100E+3 1.3199400E+0
8.3518600E+3 1.2868400E+0
8.3521100E+3 1.2568600E+0
8.3523600E+3 1.2278500E+0
8.3526100E+3 1.2022700E+0
8.3528600E+3 1.1791900E+0
8.3531100E+3 1.1594400E+0
8.3533600E+3 1.1417100E+0
8.3536100E+3 1.1265000E+0
8.3538600E+3 1.1126700E+0
8.3541100E+3 1.1002300E+0
8.3543600E+3 1.0880300E+0
8.3546100E+3 1.0759200E+0
8.3548600E+3 1.0631200E+0
8.3551100E+3 1.0488300E+0
8.3553600E+3 1.0335000E+0
8.3556100E+3 1.0173800E+0
8.3558600E+3 9.9878400E-1
8.3561100E+3 9.8044400E-1
8.3563600E+3 9.6059900E-1
8.3566100E+3 9.4066700E-1
8.3568600E+3 9.2131400E-1
8.3571100E+3 9.0189300E-1
8.3573600E+3 8.8398100E-1
8.3576100E+3 8.6682900E-1
8.3578600E+3 8.5103900E-1
8.3581100E+3 8.3749600E-1
8.3583600E+3 8.2484400E-1
8.3586100E+3 8.1439400E-1
8.3588600E+3 8.0528700E-1
8.3591100E+3 7.9847900E-1
8.3593600E+3 7.9318400E-1
8.3596100E+3 7.8957100E-1
8.3598600E+3 7.8813400E-1
8.3601100E+3 7.8808000E-1
8.3603600E+3 7.8971500E-1
8.3609900E+3 8.0202400E-1
8.3616400E+3 8.2596900E-1
8.3623100E+3 8.5818300E-1
8.3630000E+3 8.9350300E-1
8.3637100E+3 9.2290400E-1
8.3644400E+3 9.4192700E-1
8.3651800E+3 9.4571200E-1
8.3659500E+3 9.3810700E-1
8.3667400E+3 9.2156600E-1
8.3675400E+3 9.0267400E-1
8.3683700E+3 8.8543300E-1
8.3692100E+3 8.7258800E-1
8.3700800E+3 8.6317400E-1
8.3709600E+3 8.5258100E-1
8.3718600E+3 8.3965200E-1
8.3727900E+3 8.2559500E-1
8.3737200E+3 8.1350400E-1
8.3746900E+3 8.0413400E-1
8.3756700E+3 8.0016900E-1
8.3766600E+3 8.0312300E-1
8.3776800E+3 8.1336300E-1
8.3787200E+3 8.2894900E-1
8.3797800E+3 8.4796400E-1
8.3808500E+3 8.6719800E-1
8.3819500E+3 8.8352000E-1
8.3830600E+3 8.9604300E-1
8.3841900E+3 9.0548200E-1
8.3853500E+3 9.1660600E-1
8.3865200E+3 9.3600000E-1
8.3877100E+3 9.6509000E-1
8.3889200E+3 1.0026700E+0
8.3901600E+3 1.0422300E+0
8.3914100E+3 1.0783100E+0
8.3926700E+3 1.1067600E+0
8.3939700E+3 1.1268100E+0
8.3952800E+3 1.1421400E+0
8.3966000E+3 1.1557900E+0
8.3979500E+3 1.1660700E+0
8.3993200E+3 1.1669800E+0
8.4007000E+3 1.1542800E+0
8.4021100E+3 1.1288100E+0
8.4035300E+3 1.1011400E+0
8.4049700E+3 1.0739600E+0
8.4064300E+3 1.0457100E+0
8.4079200E+3 1.0158700E+0
8.4094200E+3 9.9062100E-1
8.4109400E+3 9.6821500E-1
8.4124800E+3 9.4602100E-1
8.4140400E+3 9.2551000E-1
8.4156200E+3 9.0869300E-1
8.4172100E+3 8.9747200E-1
8.4188300E+3 8.9097600E-1
8.4204700E+3 8.8991000E-1
8.4221300E+3 8.9582900E-1
8.4238000E+3 9.0717600E-1
8.4255000E+3 9.2319900E-1
8.4272100E+3 9.3989800E-1
8.4289500E+3 9.5207100E-1
8.4307000E+3 9.6026100E-1
8.4324700E+3 9.6336600E-1
8.4342600E+3 9.6671100E-1
8.4360800E+3 9.6842800E-1
8.4379000E+3 9.7300800E-1
8.4397500E+3 9.7996800E-1
8.4416200E+3 9.9194000E-1
8.4435100E+3 1.0110600E+0
8.4454100E+3 1.0316200E+0
8.4473400E+3 1.0465500E+0
8.4492900E+3 1.0513400E+0
8.4512500E+3 1.0470900E+0
8.4532400E+3 1.0357500E+0
8.4552400E+3 1.0175800E+0
8.4572600E+3 9.9366200E-1
8.4593100E+3 9.6833500E-1
8.4613700E+3 9.4282700E-1
8.4634500E+3 9.2230700E-1
8.4655500E+3 9.1051000E-1
8.4676700E+3 9.2214000E-1
8.4698100E+3 9.4227400E-1
8.4719700E+3 9.7486800E-1
8.4741500E+3 1.0078600E+0
8.4763400E+3 1.0333300E+0
8.4785600E+3 1.0431100E+0
8.4808000E+3 1.0381900E+0
8.4830600E+3 1.0241100E+0
8.4853300E+3 1.0093100E+0
8.4876200E+3 1.0006200E+0
8.4899300E+3 1.0015200E+0
8.4922700E+3 1.0094500E+0
8.4946200E+3 1.0222300E+0
8.4970000E+3 1.0324100E+0
8.4993900E+3 1.0423600E+0
8.5017900E+3 1.0490700E+0
8.5042200E+3 1.0497500E+0
8.5066800E+3 1.0445100E+0
8.5091400E+3 1.0342200E+0
8.5116300E+3 1.0190900E+0
8.5141400E+3 9.9944900E-1
8.5166600E+3 9.7498300E-1
8.5192100E+3 9.4796300E-1
8.5217700E+3 9.2438700E-1
8.5243600E+3 9.0558100E-1
8.5269600E+3 8.9613900E-1
8.5295900E+3 8.9954900E-1
8.5322200E+3 9.1551200E-1
8.5348900E+3 9.4094000E-1
8.5375700E+3 9.6935000E-1
8.5402600E+3 9.9574200E-1
8.5429900E+3 1.0177500E+0
8.5457200E+3 1.0324500E+0
8.5484900E+3 1.0402200E+0
8.5512600E+3 1.0414600E+0
8.5540600E+3 1.0382200E+0
8.5568700E+3 1.0333700E+0
8.5597100E+3 1.0283200E+0
8.5625600E+3 1.0218000E+0
8.5654300E+3 1.0162700E+0
8.5683300E+3 1.0129300E+0
8.5712400E+3 1.0112200E+0
8.5741700E+3 1.0088000E+0
8.5771300E+3 1.0046300E+0
8.5801000E+3 9.9910700E-1
8.5830900E+3 9.9421800E-1
8.5861000E+3 9.9200800E-1
8.5891300E+3 9.9364100E-1
8.5921700E+3 9.9600300E-1
8.5952400E+3 9.9530500E-1
8.5983300E+3 9.9018000E-1
8.6014300E+3 9.8197400E-1
8.6045600E+3 9.7395700E-1
8.6077100E+3 9.6857400E-1
8.6108700E+3 9.6625900E-1
8.6140500E+3 9.6746700E-1
8.6172600E+3 9.7235600E-1
8.6204700E+3 9.7982700E-1
8.6237200E+3 9.8893100E-1
8.6269800E+3 9.9928300E-1
8.6302600E+3 1.0085300E+0
8.6335600E+3 1.0157400E+0
8.6368800E+3 1.0200500E+0
8.6402200E+3 1.0221600E+0
8.6435800E+3 1.0225900E+0
8.6469500E+3 1.0222300E+0
8.6503500E+3 1.0186700E+0
8.6537600E+3 1.0091300E+0
8.6572000E+3 9.9642700E-1
8.6606500E+3 9.8512000E-1
8.6641300E+3 9.7815500E-1
8.6676200E+3 9.7714000E-1
8.6711300E+3 9.7960200E-1
8.6746600E+3 9.8372600E-1
8.6782100E+3 9.8789700E-1
8.6817800E+3 9.8875800E-1
8.6853800E+3 9.8672800E-1
8.6889800E+3 9.8488600E-1
8.6926100E+3 9.8565700E-1
8.6962500E+3 9.8993800E-1
8.6999200E+3 9.9621000E-1
8.7036100E+3 1.0017800E+0
8.7073200E+3 1.0073800E+0
8.7110400E+3 1.0127300E+0
8.7147800E+3 1.0178100E+0
8.7185400E+3 1.0213600E+0
8.7223300E+3 1.0215200E+0
8.7261300E+3 1.0192200E+0
8.7299600E+3 1.0153700E+0
8.7337900E+3 1.0108800E+0
8.7376600E+3 1.0028600E+0
8.7415300E+3 9.9247200E-1
8.7454300E+3 9.8397600E-1
8.7493500E+3 9.8112400E-1
8.7532900E+3 9.8347300E-1
8.7572500E+3 9.8849700E-1
8.7612200E+3 9.9491700E-1
8.7652100E+3 9.9964700E-1
8.7692300E+3 1.0011600E+0
8.7732600E+3 1.0001500E+0
8.7773200E+3 9.9911100E-1
8.7813900E+3 9.9962400E-1
8.7854800E+3 9.9858500E-1
8.7896000E+3 9.9895200E-1
8.7937200E+3 9.9931800E-1
8.7978800E+3 1.0015800E+0
8.8020500E+3 1.0033200E+0
8.8062300E+3 1.0051700E+0
8.8104400E+3 1.0082500E+0
8.8146700E+3 1.0124400E+0
8.8189200E+3 1.0176300E+0
8.8231800E+3 1.0195200E+0
8.8274600E+3 1.0186800E+0
8.8317700E+3 1.0169800E+0
8.8361000E+3 1.0150100E+0
8.8404400E+3 1.0136900E+0
8.8448100E+3 1.0125800E+0
8.8491900E+3 1.0111200E+0
8.8535900E+3 1.0098400E+0
8.8580100E+3 1.0077300E+0
8.8624500E+3 1.0063100E+0
8.8669000E+3 1.0068700E+0
8.8713900E+3 1.0091500E+0
8.8758800E+3 1.0108200E+0
More information about the Ifeffit
mailing list