[Ifeffit] Cu and Mn K-edge XANES
Matt Newville
newville at cars.uchicago.edu
Fri Nov 30 21:28:54 CST 2018
On Fri, Nov 30, 2018 at 6:55 PM humberto blancomanzur <huber784 at hotmail.com>
wrote:
> Dear all,
>
>
> Can somebody share any from the following XANES spectra together with the
> reference foil (any spinel composition it will be great)?
>
>
> CuO, Cu2O, Cu1.5Mn1.5O4, and Al2CuO4 (Cu K edge).
>
> MnO, MnO2, Cu1.5Mn1.5O4, and Al2MnO4 (Mn K edge).
>
>
> I will be very grateful,
>
> Humberto.
>
Some of these are available at https://millenia.cars.aps.anl.gov/xaslib/