[Ifeffit] data on CdS
Robert Gordon
ragordon at alumni.sfu.ca
Sat Nov 17 11:12:33 CST 2018
CdS Mu(E) measured in FLY on 20BM in 2013...no simultaneous reference for
energy calibration through...sorry...
On Sat, Nov 17, 2018 at 8:58 AM Anatoly Frenkel <
anatoly.frenkel at stonybrook.edu> wrote:
> Dear all - if someone could share raw Cd K-edge data of CdS, it would be
> really helpful!
> Thank you,
>
> Anatoly Frenkel
>
> _______________________________________________
> Ifeffit mailing list
> Ifeffit at millenia.cars.aps.anl.gov
> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
> Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20181117/17e6c2b0/attachment.html>
-------------- next part --------------
# created: Sat Nov 17 09:09:50 2018
# from file: CdS.0001
# No: 188 [E0: 0,0,0,-1]
#---------------------------------------------------------------------
# X Y
2.6509967484E+001 8.1981685849E-002
2.6522966218E+001 8.2039334847E-002
2.6530709632E+001 8.2314242540E-002
2.6540937882E+001 8.2622455830E-002
2.6551174044E+001 8.2973458220E-002
2.6559710229E+001 8.3025571378E-002
2.6569184074E+001 8.3467073750E-002
2.6581774578E+001 8.3868808081E-002
2.6590330509E+001 8.4288477980E-002
2.6599203394E+001 8.4907020243E-002
2.6610731441E+001 8.5616716176E-002
2.6619150126E+001 8.6300952848E-002
2.6627262057E+001 8.6950411767E-002
2.6640064027E+001 8.8519836354E-002
2.6650377022E+001 9.0255058520E-002
2.6657413200E+001 9.1903286891E-002
2.6669618074E+001 9.5520286690E-002
2.6678857412E+001 1.0088238447E-001
2.6680110698E+001 1.0198841339E-001
2.6681364102E+001 1.0322150882E-001
2.6682460927E+001 1.0426791489E-001
2.6683244429E+001 1.0493911662E-001
2.6684654849E+001 1.0604903078E-001
2.6686065418E+001 1.0755723314E-001
2.6687476137E+001 1.0934065869E-001
2.6688573467E+001 1.1087268087E-001
2.6690611604E+001 1.1427757282E-001
2.6692493239E+001 1.1804216394E-001
2.6694845656E+001 1.2372363963E-001
2.6696727890E+001 1.2964421093E-001
2.6698296621E+001 1.3574892067E-001
2.6700179342E+001 1.4467003583E-001
2.6702533118E+001 1.5907707229E-001
2.6704259485E+001 1.7492482873E-001
2.6705829104E+001 1.9376857997E-001
2.6707555899E+001 2.2456050148E-001
2.6709282917E+001 2.7488813854E-001
2.6710539071E+001 3.2931696535E-001
2.6712109430E+001 4.3075370795E-001
2.6712580574E+001 4.6509710082E-001
2.6713837039E+001 5.5121353203E-001
2.6714936543E+001 6.1890272150E-001
2.6716036138E+001 6.5795641989E-001
2.6716664519E+001 6.6843613404E-001
2.6718235601E+001 6.7225107612E-001
2.6719649732E+001 6.6655205452E-001
2.6721535475E+001 6.6061722896E-001
2.6723421484E+001 6.5649047122E-001
2.6724993363E+001 6.5310683840E-001
2.6727351529E+001 6.4541413355E-001
2.6729238361E+001 6.3828502209E-001
2.6731282732E+001 6.3337999943E-001
2.6732226393E+001 6.3225437205E-001
2.6734428529E+001 6.3335050642E-001
2.6735687056E+001 6.3476376759E-001
2.6737260382E+001 6.3454468468E-001
2.6738047115E+001 6.3393243290E-001
2.6739620719E+001 6.3098467813E-001
2.6740879736E+001 6.2698790960E-001
2.6742296273E+001 6.2249491618E-001
2.6743398127E+001 6.1792551178E-001
2.6744500073E+001 6.1348949344E-001
2.6745759551E+001 6.0889801897E-001
2.6747019148E+001 6.0478409463E-001
2.6748121393E+001 6.0208260371E-001
2.6750011168E+001 6.0155902348E-001
2.6751428675E+001 6.0439296087E-001
2.6753633985E+001 6.1351230405E-001
2.6755997221E+001 6.2628389052E-001
2.6758360877E+001 6.3937595288E-001
2.6761355441E+001 6.5242180872E-001
2.6763720046E+001 6.5837225603E-001
2.6766085070E+001 6.6059608871E-001
2.6769081369E+001 6.6041714557E-001
2.6771289598E+001 6.6088373790E-001
2.6773340424E+001 6.6188678594E-001
2.6774918197E+001 6.6274593239E-001
2.6776653963E+001 6.6298172944E-001
2.6778232127E+001 6.6216000409E-001
2.6779652635E+001 6.5963284561E-001
2.6781389016E+001 6.5530383783E-001
2.6784388752E+001 6.4580959676E-001
2.6787073297E+001 6.3811933114E-001
2.6790232276E+001 6.3077951179E-001
2.6793392003E+001 6.2572489506E-001
2.6796078358E+001 6.2306216403E-001
2.6798765254E+001 6.2167471876E-001
2.6800820303E+001 6.2241307189E-001
2.6803191907E+001 6.2596301819E-001
2.6805722081E+001 6.3040575480E-001
2.6807620026E+001 6.3462053538E-001
2.6809834636E+001 6.3976111639E-001
2.6812524299E+001 6.4497026040E-001
2.6815689301E+001 6.5023435444E-001
2.6819646607E+001 6.5436640485E-001
2.6823288363E+001 6.5705648242E-001
2.6826614311E+001 6.5852209889E-001
2.6830416408E+001 6.5977256730E-001
2.6833744128E+001 6.5956529809E-001
2.6836755637E+001 6.5919095135E-001
2.6838975077E+001 6.5818621906E-001
2.6841194885E+001 6.5563669923E-001
2.6843256465E+001 6.5367315379E-001
2.6846270114E+001 6.5041510566E-001
2.6850395156E+001 6.4598020656E-001
2.6854521469E+001 6.4170329136E-001
2.6858172729E+001 6.3861638675E-001
2.6861507358E+001 6.3717631457E-001
2.6864683966E+001 6.3682696907E-001
2.6867543559E+001 6.3740348384E-001
2.6870403761E+001 6.3774856792E-001
2.6873105625E+001 6.3855983608E-001
2.6876125999E+001 6.3981492308E-001
2.6879942182E+001 6.4206780961E-001
2.6883918528E+001 6.4468073813E-001
2.6888532568E+001 6.4709369381E-001
2.6892989010E+001 6.4814273605E-001
2.6897287697E+001 6.4929241810E-001
2.6900950628E+001 6.4931014526E-001
2.6903658655E+001 6.4952261345E-001
2.6906048545E+001 6.4961708113E-001
2.6910032640E+001 6.4902566099E-001
2.6914974562E+001 6.4775431480E-001
2.6919439798E+001 6.4638685978E-001
2.6924066073E+001 6.4441013859E-001
2.6927576725E+001 6.4224298104E-001
2.6930928658E+001 6.4100021864E-001
2.6934441104E+001 6.4031694669E-001
2.6937315607E+001 6.3871621207E-001
2.6941788280E+001 6.3683649600E-001
2.6947061556E+001 6.3566458420E-001
2.6952177014E+001 6.3514780197E-001
2.6957294419E+001 6.3532038931E-001
2.6962413773E+001 6.3603066795E-001
2.6965934460E+001 6.3693573528E-001
2.6968975795E+001 6.3787092872E-001
2.6972658332E+001 6.3911900884E-001
2.6977943734E+001 6.3956568380E-001
2.6982910700E+001 6.3945364187E-001
2.6987719188E+001 6.3972614864E-001
2.6991727575E+001 6.3934633222E-001
2.6995416345E+001 6.3956816335E-001
2.6998945680E+001 6.3975422380E-001
2.7002796919E+001 6.3953592709E-001
2.7008415284E+001 6.3833606020E-001
2.7013875370E+001 6.3686674004E-001
2.7019659051E+001 6.3575244500E-001
2.7025445215E+001 6.3418395813E-001
2.7029786470E+001 6.3405330521E-001
2.7033003115E+001 6.3385241469E-001
2.7037346805E+001 6.3283977414E-001
2.7043462517E+001 6.3131371430E-001
2.7049419956E+001 6.3117883484E-001
2.7054252244E+001 6.3100502486E-001
2.7058441628E+001 6.3158741008E-001
2.7062793519E+001 6.3160030983E-001
2.7067630600E+001 6.3209121896E-001
2.7073760059E+001 6.3256243191E-001
2.7079408076E+001 6.3202722359E-001
2.7085704364E+001 6.3242933858E-001
2.7091357380E+001 6.3295841554E-001
2.7095558295E+001 6.3299077574E-001
2.7099598868E+001 6.3254587320E-001
2.7106066299E+001 6.3240494079E-001
2.7112051429E+001 6.3169163802E-001
2.7117715479E+001 6.3089532940E-001
2.7122410346E+001 6.3102599445E-001
2.7126458954E+001 6.3047562483E-001
2.7131156857E+001 6.3029391440E-001
2.7137963611E+001 6.2937285413E-001
2.7144287235E+001 6.2836034123E-001
2.7151100597E+001 6.2775471720E-001
2.7156943352E+001 6.2859831975E-001
2.7161327073E+001 6.2852072528E-001
2.7166849334E+001 6.2827133899E-001
2.7173836594E+001 6.2802249843E-001
2.7180339607E+001 6.2770933194E-001
2.7185544265E+001 6.2852414677E-001
2.7190262713E+001 6.2862669347E-001
2.7195633979E+001 6.2908224602E-001
2.7202798978E+001 6.2909111805E-001
2.7209315899E+001 6.2912210532E-001
2.7216488130E+001 6.2873011908E-001
2.7222522259E+001 6.2860952771E-001
2.7226927235E+001 6.2910889493E-001
2.7233455754E+001 6.2897351846E-001
2.7240640752E+001 6.2812549008E-001
2.7247502706E+001 6.2765115627E-001
More information about the Ifeffit
mailing list