[Ifeffit] data on CdS
Ravel, Bruce
bravel at bnl.gov
Sat Nov 17 11:10:49 CST 2018
There are a bunch of Cd standards that come with Demeter.
https://github.com/bruceravel/demeter/blob/master/lib/Demeter/share/standards/data/Cd.prj
Click on the "Download" button and save the prj file.
CdS is in there, along with sulphate, carbonate, nitrate, hydroxide and
metal. I measured them at APS 10ID about 13 years ago with some of Don
Spark's (then) students.
B
On 11/17/2018 11:56 AM, Anatoly Frenkel wrote:
> Dear all - if someone could share raw Cd K-edge data of CdS, it would be
> really helpful!
> Thank you,
>
> Anatoly Frenkel
>
>
>
> _______________________________________________
> Ifeffit mailing list
> Ifeffit at millenia.cars.aps.anl.gov
> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
> Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit
>
--
Bruce Ravel ------------------------------------ bravel at bnl.gov
National Institute of Standards and Technology
Synchrotron Science Group at NSLS-II
Lead Beamline Scientist, 6BM (BMM)
Building 743, Room 114
Upton NY, 11973
Homepage: http://bruceravel.github.io/home/
Beamline: https://www.bnl.gov/ps/beamlines/beamline.php?r=6-BM
Software: https://github.com/bruceravel
Demeter: http://bruceravel.github.io/demeter/
More information about the Ifeffit
mailing list