[Ifeffit] Athena (Demeter 0.9.26) does not import all datapoints from ascci file
Prüßmann, Tim (IKFT)
tim.pruessmann at kit.edu
Mon Mar 26 09:32:17 CDT 2018
Hi,
I can confirm Kathy's problem.
On my computer with Athena (Demeter 0.9.26) only 109 of 275 points are imported.
Reinstalling Demeter 0.9.25 fixes the problem again.
Tim
From: Ifeffit [mailto:ifeffit-bounces at millenia.cars.aps.anl.gov] On Behalf Of Kathy Dardenne
Sent: Wednesday, February 28, 2018 9:19 PM
To: ifeffit at millenia.cars.aps.anl.gov
Subject: [Ifeffit] Athena (Demeter 0.9.26) does not import all datapoints from ascci file
Hello,
I got a new trouble by importing datafile in Athena (Demeter 0.9.26).
Athena from Demeter version 0.9.26 does not import all points from the datafile but some of them yielding a very poor resolution especially for the edge region.
The given file has 275 points and only 143points are imported (see derivative after import with Athena(26) and with pymca were all points are imported).
Importing data using Athena from an older version of Demeter and saving the file solved my import problem temporary. But there I notice that a priori only 202 instead 275 were imported but it was not obvious from the plot appearance that some points are missing .
I joined some screenshots as well as Athena log file after importing the data (error message about a file not found but the name in stash is not the one Athena is looking for....?). I joined both Athena file (Demeter v26 and Demeter v19 after import of the same asci file) as well as the asci file. I got the problem of "partial import" with all my datafiles.
Did somebody experienced this trouble too?
Thanks a lot
Kathy Dardenne
Operating system : Windows 7 entreprise - Service pack 1
Programme : Demeter 0.9.26 last release
Karlsruhe Institute of Technology (KIT)
Institute for nuclear waste disposal (INE)
Dr. Kathy DARDENNE
Hermann-von-Helmholtz-Platz 1,
Building 712
76344 Eggenstein-Leopoldshafen, Germany
Tel. : +49 721 608-26669
Fax : +49 721 608-23927
E-mail : dardenne at kit.edu<mailto:kathy.dardenne at kit.edu>
Internet : www.ine.kit.edu<http://www.kit.edu/>
KIT - The Research University in the Helmholtz Association.
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20180326/a3532450/attachment-0001.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: Zr_calib_athena25.PNG
Type: image/png
Size: 34171 bytes
Desc: Zr_calib_athena25.PNG
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20180326/a3532450/attachment-0003.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: Zr_calib_athena26.PNG
Type: image/png
Size: 36909 bytes
Desc: Zr_calib_athena26.PNG
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20180326/a3532450/attachment-0004.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: Zr_calib_athena26_deriv.PNG
Type: image/png
Size: 42171 bytes
Desc: Zr_calib_athena26_deriv.PNG
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20180326/a3532450/attachment-0005.png>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: dathena_26.log
Type: application/octet-stream
Size: 881 bytes
Desc: dathena_26.log
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20180326/a3532450/attachment-0002.obj>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: dathena_25.log
Type: application/octet-stream
Size: 1029 bytes
Desc: dathena_25.log
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20180326/a3532450/attachment-0003.obj>
More information about the Ifeffit
mailing list