Dear Colleagues,
I am aiming to use Larch to synthesise EXAFS spectra for metal oxides and I
wonder if that would be the right way. I can synthesise the paths in
Demeter/Artemis but I have no idea how to sum them in order to obtain a
single EXAFS spectrum. Hence, the interest in Larch hoping that it can do
what I am looking for.
Best regards,
Kate