[Ifeffit] FeSe2 Se K-edge XANES request
Yasin Deep
yasindeep at gmail.com
Wed Mar 14 12:34:22 CDT 2018
For Te doped FeSe we have this paper. If you have any questions do not
hesitate to communicate.
With Bests,
Yasin
14 Mar 2018 Çar 20:17 tarihinde Anatoly Frenkel <
anatoly.frenkel at stonybrook.edu> şunu yazdı:
> Will the data from the compositions shown in this paper be useful?
>
>
> https://cpb-us-east-1-juc1ugur1qwqqqo4.stackpathdns.com/you.stonybrook.edu/dist/b/1881/files/2016/10/BaFeSe-EXAFS-y9zet9.pdf
>
> Anatoly
>
> Hi Folks,
>>
>> Does anyone have a near-edge spectrum of FeSe2, Se K-edge, they could
>> share?
>> (Ideally with Se elemental reference measured simultaneous.)
>>
>> Thanks,
>> -R.
>> _______________________________________________
>> Ifeffit mailing list
>> Ifeffit at millenia.cars.aps.anl.gov
>> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
>> Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit
>>
>
> _______________________________________________
> Ifeffit mailing list
> Ifeffit at millenia.cars.aps.anl.gov
> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
> Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20180314/b8e39fca/attachment-0001.html>
-------------- next part --------------
A non-text attachment was scrubbed...
Name: c5cp01740h.pdf
Type: application/pdf
Size: 2261290 bytes
Desc: not available
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20180314/b8e39fca/attachment-0001.pdf>
More information about the Ifeffit
mailing list