[Ifeffit] Cu and Mn K-edge XANES
humberto blancomanzur
huber784 at hotmail.com
Sat Dec 1 06:03:00 CST 2018
Thank you so much for the help Matt,
now I just need the spinel phases:
Cu1.5Mn1.5O4, and Al2CuO4 (Cu K edge).
Cu1.5Mn1.5O4, and Al2MnO4 (Mn K edge).
Humberto.
________________________________
De: Ifeffit <ifeffit-bounces at millenia.cars.aps.anl.gov> em nome de Matt Newville <newville at cars.uchicago.edu>
Enviado: sábado, 1 de dezembro de 2018 01:28
Para: XAFS Analysis using Ifeffit
Assunto: Re: [Ifeffit] Cu and Mn K-edge XANES
On Fri, Nov 30, 2018 at 6:55 PM humberto blancomanzur <huber784 at hotmail.com<mailto:huber784 at hotmail.com>> wrote:
Dear all,
Can somebody share any from the following XANES spectra together with the reference foil (any spinel composition it will be great)?
CuO, Cu2O, Cu1.5Mn1.5O4, and Al2CuO4 (Cu K edge).
MnO, MnO2, Cu1.5Mn1.5O4, and Al2MnO4 (Mn K edge).
I will be very grateful,
Humberto.
Some of these are available at https://millenia.cars.aps.anl.gov/xaslib/
--Matt
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20181201/31a2e12e/attachment-0001.html>
More information about the Ifeffit
mailing list