[Ifeffit] Ifeffit Digest, Vol 153, Issue 11
Marcelo Eduardo Alves
mealves at gmail.com
Mon Nov 9 12:58:25 CST 2015
I have downloaded the zip-file containing the example files and extracted
them into other subfolders (i.e. C:\Users\Marcelo\Documents\1.Athena
Calibração e Alinhamento\Examples\Fe foil).
When I use C:\Fe foil the file was opened in Athena without any issue.
Thank you.
2015-11-09 15:55 GMT-02:00 <ifeffit-request at millenia.cars.aps.anl.gov>:
> Send Ifeffit mailing list submissions to
> ifeffit at millenia.cars.aps.anl.gov
>
> To subscribe or unsubscribe via the World Wide Web, visit
> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
> or, via email, send a message with subject or body 'help' to
> ifeffit-request at millenia.cars.aps.anl.gov
>
> You can reach the person managing the list at
> ifeffit-owner at millenia.cars.aps.anl.gov
>
> When replying, please edit your Subject line so it is more specific
> than "Re: Contents of Ifeffit digest..."
>
>
> Today's Topics:
>
> 1. Demeter under El Capitan (Fowler, Joseph W.)
> 2. Re: Demeter under El Capitan (Zack Gainsforth)
> 3. Opening "older" data files in the latest Athena version
> (Marcelo Eduardo Alves)
> 4. Re: Opening "older" data files in the latest Athena version
> (Bruce Ravel)
>
>
> ----------------------------------------------------------------------
>
> Message: 1
> Date: Mon, 9 Nov 2015 16:20:09 +0000
> From: "Fowler, Joseph W." <joe.fowler at nist.gov>
> To: "ifeffit at millenia.cars.aps.anl.gov"
> <ifeffit at millenia.cars.aps.anl.gov>
> Subject: [Ifeffit] Demeter under El Capitan
> Message-ID: <CAAD97E1-600B-43B3-B7AE-FAE9E373DC3E at nist.gov>
> Content-Type: text/plain; charset="windows-1252"
>
> Bruce, Scott, Manuel:
>
> I?m the MacPorts maintainer for demeter and ifeffit, but I?m afraid I have
> not been much help lately.
>
> I?m sorry that I have not chimed in about any of the recent reports Mac /
> Macports problems under El Capitan. It so happens that my employer (US
> National Institute of Standards and Technology) does not let us upgrade to
> Yosemite OR El Capitan. They own the only Macs to which I have access, so I
> can only work under Mavericks. I?m afraid that artemis, hephaestus, and
> athena all start properly for me.
>
> To Manuel from Grenoble, all I can say is that xorg-server has a lot of
> dependencies, and it will take a long time to install the needed ports the
> first time. I would not think an entire hour is out of the question,
> depending on your connection speed and computer performance.
>
> To the others having trouble running (as opposed to installing), I wonder
> if anyone in the community is having success with the demeter suite under
> El Capitan? If so, we?d all be grateful if you could let us know what
> tricks were required. I am totally helpless on OS 10.10 and 10.11-specific
> problems.
>
> Joe Fowler
> NIST Boulder Laboratories
>
>
> -------------- next part --------------
> An HTML attachment was scrubbed...
> URL: <
> http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20151109/3d40166e/attachment-0001.htm
> >
>
> ------------------------------
>
> Message: 2
> Date: Mon, 9 Nov 2015 09:43:56 -0800
> From: Zack Gainsforth <zackg at berkeley.edu>
> To: XAFS Analysis using Ifeffit <ifeffit at millenia.cars.aps.anl.gov>
> Subject: Re: [Ifeffit] Demeter under El Capitan
> Message-ID: <1684C2DE-100F-49E4-A578-E4C1F740CDFE at berkeley.edu>
> Content-Type: text/plain; charset="windows-1252"
>
> I am running under El Capitan and previously under Yosemite. I didn?t
> really have trouble with the installation, though I do note that after you
> upgrade the OS, you need to reinstall ALL of macports from scratch
> sometimes. That means nuke the old directory, download macports from the
> website and install it and then install each package. And have patience,
> it can take hours to install all dependencies. I usually let it run
> overnight.
>
> I?m also using XQuartz.
>
> Macports has documentation about doing this:
>
> https://trac.macports.org/wiki/Migration <
> https://trac.macports.org/wiki/Migration>
>
> and if that fails:
>
> https://guide.macports.org/chunked/installing.macports.uninstalling.html <
> https://guide.macports.org/chunked/installing.macports.uninstalling.html>
>
> I would try reinstall first, and then if there is still trouble, dig
> deeper.
>
> Zack
>
> (Note, I?ve only used Hephaestus and Athena on El Capitan. But Artemis
> worked for me on Yosemite.)
>
> > On Nov 9, 2015, at 8:20 AM, Fowler, Joseph W. <joe.fowler at nist.gov>
> wrote:
> >
> > Bruce, Scott, Manuel:
> >
> > I?m the MacPorts maintainer for demeter and ifeffit, but I?m afraid I
> have not been much help lately.
> >
> > I?m sorry that I have not chimed in about any of the recent reports Mac
> / Macports problems under El Capitan. It so happens that my employer (US
> National Institute of Standards and Technology) does not let us upgrade to
> Yosemite OR El Capitan. They own the only Macs to which I have access, so I
> can only work under Mavericks. I?m afraid that artemis, hephaestus, and
> athena all start properly for me.
> >
> > To Manuel from Grenoble, all I can say is that xorg-server has a lot of
> dependencies, and it will take a long time to install the needed ports the
> first time. I would not think an entire hour is out of the question,
> depending on your connection speed and computer performance.
> >
> > To the others having trouble running (as opposed to installing), I
> wonder if anyone in the community is having success with the demeter suite
> under El Capitan? If so, we?d all be grateful if you could let us know what
> tricks were required. I am totally helpless on OS 10.10 and 10.11-specific
> problems.
> >
> > Joe Fowler
> > NIST Boulder Laboratories
> >
> >
> > _______________________________________________
> > Ifeffit mailing list
> > Ifeffit at millenia.cars.aps.anl.gov
> > http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
> > Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit
>
> -------------- next part --------------
> An HTML attachment was scrubbed...
> URL: <
> http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20151109/4497d87e/attachment-0001.htm
> >
>
> ------------------------------
>
> Message: 3
> Date: Mon, 9 Nov 2015 15:46:08 -0200
> From: Marcelo Eduardo Alves <mealves at gmail.com>
> To: ifeffit at millenia.cars.aps.anl.gov
> Subject: [Ifeffit] Opening "older" data files in the latest Athena
> version
> Message-ID:
> <CAAO6x+aQRQOe61_=451mSNJD=
> NdcY2C0NmkFNmbiojbx5Lcp6Q at mail.gmail.com>
> Content-Type: text/plain; charset="utf-8"
>
> I have downloaded the worked examples available at
> https://github.com/bruceravel/XAS-Education
>
> However, I am not being able to open them in the latest Athena version
> (0.9.24) (e.g., Fe.060 of Fe foil folder).
>
> Could those files be opened in the last Athena version?
>
> Thank you.
>
> Marcelo.
> -------------- next part --------------
> An HTML attachment was scrubbed...
> URL: <
> http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20151109/c9fad590/attachment-0001.htm
> >
>
> ------------------------------
>
> Message: 4
> Date: Mon, 9 Nov 2015 12:55:21 -0500
> From: Bruce Ravel <bravel at bnl.gov>
> To: XAFS Analysis using Ifeffit <ifeffit at millenia.cars.aps.anl.gov>
> Subject: Re: [Ifeffit] Opening "older" data files in the latest Athena
> version
> Message-ID: <5640DE09.4080306 at bnl.gov>
> Content-Type: text/plain; charset=windows-1252; format=flowed
>
> On 11/09/2015 12:46 PM, Marcelo Eduardo Alves wrote:
> > I have downloaded the worked examples available at
> > https://github.com/bruceravel/XAS-Education
> >
> > However, I am not being able to open them in the latest Athena version
> > (0.9.24) (e.g., Fe.060 of Fe foil folder).
> >
> > Could those files be opened in the last Athena version?
>
> Yes. No problems here on any of my computers.
>
> Here are some hints on how to ask a question effectively:
>
> http://bruceravel.github.com/demeter/pods/bugs.pod.html
> http://bruceravel.github.com/demeter/pods/help.pod.html
>
> B
>
> --
> Bruce Ravel ------------------------------------ bravel at bnl.gov
>
> National Institute of Standards and Technology
> Synchrotron Science Group at NSLS-II
> Building 535A
> Upton NY, 11973
>
> Homepage: http://bruceravel.github.io/home/
> Software: https://github.com/bruceravel
> Demeter: http://bruceravel.github.io/demeter/
>
>
> ------------------------------
>
> _______________________________________________
> Ifeffit mailing list
> Ifeffit at millenia.cars.aps.anl.gov
> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
> Unsubscribe: http://millenia.cars.aps.anl.gov/mailman/options/ifeffit
>
>
> End of Ifeffit Digest, Vol 153, Issue 11
> ****************************************
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20151109/094d2af5/attachment.html>
More information about the Ifeffit
mailing list