Hi everyone,
I'm somewhat new to EXAFS and this is my first question for the Ifeffit mailing list (which is a great source of information by the way).I was reading the excellent paper: "Path degeneracy and EXAFS analysis of disordered materials" and I have a "simple" question to ask:How do I get from table 1 to table 2?
Specifically, I think I know how to use fuzzy degeneracy in Artemis for the paths in one FEFF calculation, but in this case there are 3 sites for Ti, and that means 3 FEFF calculations (rigth?).
So how do I use fuzzy degeneracy for paths from different FEFF calculations?
And by the way, is it right if I imagine the material as having only 1 "fuzzy"/average site for Ti?
Thanks in advance
Juan
****************************** ****************************** ****************************** *********Dr. Juan Manuel Conde GarridoLaboratorio de Sólidos AmorfosDepartameno de Física, Facultad de Ingeniería, Universidad de Buenos Aires
INTECIN (UBA-CONICET)
Av. Paseo Colón 850
C1063ACV - Ciudad de Buenos Aires
ARGENTINA
Tel: +54 (11) 4343-0893/4343-0092 (Int. 1101)
http://intecin.fi.uba.ar
****************************** ****************************** ****************************** *********
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20150619/8252a229/attachment.html>
More information about the Ifeffit
mailing list