[Ifeffit] Mn3O4 EXAFS fitting
Scott Calvin
scalvin at sarahlawrence.edu
Tue Jun 2 07:15:56 CDT 2015
Thanks, Kug-Seung. If you have the book, a spinel is one of the case studies in the last chapter! If you flip to section 16.4, that might provide additional help.
—Scott Calvin
Sarah Lawrence College
On Jun 1, 2015, at 9:43 PM, 이국승 <lks3006 at postech.ac.kr<mailto:lks3006 at postech.ac.kr>> wrote:
Dear Scott,
In addition to practical explanation from Fred, you give theoretical details and a good example.
I am reading your book 'XAFS for everyone' from time to time. It helps a lot.
Thank you.
Kug-Seung Lee