Dear All,
Suppose I have a compound, say AB. I have the EXAFS data from both A-edge
as well as B-edge and I am simultaneously refining these data.
Would it be correct to force the mean square displacement of the A-B path
in both the edges to be the same?
-- Regards,
Badari Narayana. A. R.
Ph.D Student, Nanoscience and Nanotechnology,
c/o Prof Rajeev Ranjan,
Electroceramics Lab,
Department of Materials Engineering,
Indian Institute of Science.