Hello All,

If I have a Ta(1-x)Ge(x)O(y) thin film, with Germanium concentration
of a few percent, is it possible in principle to get useable
fluorescence-mode EXAFS spectra around the Ge K edge (11.1 keV)? Or is
it likely that the spectra would be complicated by additional Ge
fluorescence excited by processes triggered by Tantalum L edge
absorption (9.88, 11.13, 11.68 keV)?