[Ifeffit] Artemis in Demeter 0.9.17 Crashing Upon Loading Project File
Anthony Ardizzi
anthony.ardizzi at gmail.com
Wed Jul 17 11:23:20 CDT 2013
Thanks Bruce. Glad I could assist in my own small way.
Anthony
On Wed, Jul 17, 2013 at 7:40 AM, Bruce Ravel <bravel at bnl.gov> wrote:
>
> Anthony,
>
> I observe the same behavior you report. In fact, the thing you are
> reporting is only a symptom of a bigger problem in how Artemis
> writes in project files -- something I had never noticed before.
>
> Thanks for this bug report. I am really grateful -- the software only
> gets better thanks to this sort of feedback. Hopefully, I will be
> able to fix this for the upcoming release.
>
> To get you over the immediate hurdle, I am attaching a project file
> containing only the most recent fit and none of the rest of the
> history. It should open without trouble and allow you to continue
> making progress.
>
> B
>
>
>
> On 07/16/2013 02:17 PM, Anthony Ardizzi wrote:
>
>> Dear Bruce and Ifeffit mailing list,
>>
>> I have just started experiencing a program crash in Artemis while trying
>> to load a project I am working on. I am performing a fit on Sr2IrO4
>> data, and when I try to open the project file, it starts loading all of
>> the usual stuff, and then when it gets to loading the path-lists/data
>> sets screen for one of the two data sets I have, the entire program
>> simply closes.
>>
>> I have attached both my project file, as well as the dartemis log file.
>> I believe the relevant error in the log file is "Illegal division by
>> zero at C:/strawberry/perl/site/lib/**Demeter/Data.pm line 922." I am
>> running Windows 7 64-bit.
>>
>> Thanks for any help you can provide,
>> Anthony
>>
>>
>> ______________________________**_________________
>> Ifeffit mailing list
>> Ifeffit at millenia.cars.aps.anl.**gov <Ifeffit at millenia.cars.aps.anl.gov>
>> http://millenia.cars.aps.anl.**gov/mailman/listinfo/ifeffit<http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit>
>>
>>
>
> --
> Bruce Ravel ------------------------------**------ bravel at bnl.gov
>
> National Institute of Standards and Technology
> Synchrotron Methods Group at NSLS --- Beamlines U7A, X24A, X23A2
> Building 535A
> Upton NY, 11973
>
> Homepage: http://xafs.org/BruceRavel
> Software: https://github.com/bruceravel
>
> _______________________________________________
> Ifeffit mailing list
> Ifeffit at millenia.cars.aps.anl.gov
> http://millenia.cars.aps.anl.gov/mailman/listinfo/ifeffit
>
>
-------------- next part --------------
An HTML attachment was scrubbed...
URL: <http://millenia.cars.aps.anl.gov/pipermail/ifeffit/attachments/20130717/87d41add/attachment.html>
More information about the Ifeffit
mailing list